MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Vestamid® X7393 sw (dry properties) Nylon 12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Uses: Flexible tubing and hoses for automobile construction according to DIN 73 378 and DIN 74 324, Type: PA 12-PHLY.

ISO data as provided by the manufacturer.

Key Words: Polyamide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³
Moisture Absorption at Equilibrium <= 0.50 %<= 0.50 %Humidity Absorption
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 31.0 MPa4500 psi
Elongation at Break >= 50 %>= 50 %
Elongation at Yield 28 %28 %
Modulus of Elasticity 0.580 GPa84.1 ksi
Charpy Impact Unnotched NBNB
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Charpy Impact, Notched NBNB
 0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cm
Dielectric Constant  4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
 10
@Frequency 100 Hz
10
@Frequency 100 Hz
Dielectric Strength 27.0 kV/mm686 kV/in
Dissipation Factor  0.11
@Frequency 1e+6 Hz
0.11
@Frequency 1e+6 Hz
 0.19
@Frequency 100 Hz
0.19
@Frequency 100 Hz
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Temperature 20.0 °C
55.6 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow 100 µm/m-°C
@Temperature 20.0 °C
55.6 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 115 °C239 °F
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °F
Vicat Softening Point 130 °C266 °F50°C/hr/50 N
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Vestamid® X7393 Plasticized Nylon 12
Evonik Vestamid® L2123 Plasticized Nylon 12
Evonik Vestamid® L2140 sw 9.7504 (dry properties) Nylon 12
Evonik Vestamid® LX9013 Plasticized Nylon 12
Evonik Vestamid® L2140 sw 9.7504 (as-conditioned) Nylon 12

PHUL99 / 47359

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.