MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

California Fine Wire Nickel 211 (Nickel Manganese Alloy)
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: All values may vary dependent on specific design and usage

Capabilities:

  • Wire
  • Ribbon
  • Square
  • Insulated
  • Plated

Information provided by California Fine Wire.

Key Words: ASTM F290
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.72 g/cc0.315 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 517 MPa75000 psiAnnealed
 793 MPa115000 psiStress relieved
 965 MPa140000 psiHard
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000170 ohm-cm0.0000170 ohm-cm3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 49.3 W/m-K342 BTU-in/hr-ft²-°F
Melting Point 1430 °C2610 °F
Maximum Service Temperature, Air 500 °C932 °FOperating Temperature
 
Component Elements PropertiesMetricEnglishComments
Manganese, Mn 4.75 %4.75 %
Nickel, Ni 93.7 %93.7 %
 
Descriptive Properties
MagneticStrong
Temperature Coefficient of Resistance0.0032 ohms/ohm-°C0-100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals Nickel 200
Special Metals Nickel 201
Special Metals Nickel 205
Alloy 19® Thermocouple Alloy
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated

NCALZ03 / 15546

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.