MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

Special Metals Nickel 205  (discontinued **)
Categories: Metal; Nonferrous Metal; Nickel Alloy; Pure Element

Material Notes: Wrought nickel similar to Nickel 200 but with compositional adjustments to enhance performance in electrical and electronic applications. Ferromagnetic. Used for the anodes and grids of electronic valves, magnetostrictive transducers, lead wires, transistor housings, and battery cases. Standard product forms are sheet, strip and wire.

Data provided by the manufacturer, Special Metals.

Key Words: Nickel, Ni, UNS N02205; ASTM F1, F2, F3, F9; SAE AMS 5555; MIL-N-46025; Werkstoff Nr. 2.4061
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 345 MPa50000 psiAnnealed
Tensile Strength, Yield 90.0 MPa
@Strain 0.2 %
13100 psi
@Strain 0.2 %
Annealed
Elongation at Break 45 %45 %Annealed
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000950 ohm-cm0.00000950 ohm-cm
Curie Temperature 360 °C680 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.3 µm/m-°C
@Temperature 20.0 - 100 °C
7.39 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.456 J/g-°C0.109 BTU/lb-°F
Thermal Conductivity 75.0 W/m-K521 BTU-in/hr-ft²-°F
Melting Point 1435 - 1446 °C2615 - 2635 °F
Solidus 1435 °C2615 °F
Liquidus 1446 °C2635 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Copper, Cu <= 0.15 %<= 0.15 %
Iron, Fe <= 0.20 %<= 0.20 %
Magnesium, Mg 0.010 - 0.080 %0.010 - 0.080 %
Manganese, Mn <= 0.35 %<= 0.35 %
Nickel, Ni >= 99 %>= 99 %Including Cobalt
Silicon, Si <= 0.15 %<= 0.15 %
Sulfur, S <= 0.0080 %<= 0.0080 %
Titanium, Ti 0.010 - 0.050 %0.010 - 0.050 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals Nickel 200
Special Metals Nickel 201
MetalTek MTEK CZ-100 Cast UNS N02100 Severe Corrosion and Heat Resistant Alloy
Special Metals Nickel 270
Universal Wire Works 99 Nickel Alloy Welding Wire

NINC02 / 17389

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.