MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

309 Stainless Steel, annealed, plate
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Key Words: UNS S30900, ASME SA249, ASME SA312, ASME SA358, ASME SA403, ASME SA409, ASTM A167, ASTM A249, ASTM A312, ASTM A314, ASTM A358, ASTM A403, ASTM A409, ASTM A473, ASTM A511, ASTM A554, ASTM A580, FED QQ-S-763, FED QQ-S-766, MIL SPEC MIL-S-862, SAE J405 (30309), DIN 1.4828, X15CrNiSi2012, UNI X 16 CrNi 23 14, B.S. 309 S 24, PN 86022 (Poland), H20N13S2, austenitic
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 170170
Hardness, Knoop 191191Converted from Brinell
Hardness, Rockwell B 8686Converted from Brinell
Hardness, Vickers 178178Converted from Brinell
Tensile Strength, Ultimate 655 MPa95000 psi
Tensile Strength, Yield 275 MPa
@Strain 0.2 %
39900 psi
@Strain 0.2 %
Elongation at Break 45 %45 %in 50 mm
Modulus of Elasticity 200 GPa29000 ksi
Poissons Ratio 0.300.30
Shear Modulus 77.0 GPa11200 ksi
Izod Impact 120 - 165 J88.5 - 122 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000780 ohm-cm
@Temperature 20.0 °C
0.0000780 ohm-cm
@Temperature 68.0 °F
Magnetic Permeability 1.0081.008at RT
 
Thermal PropertiesMetricEnglishComments
CTE, linear  14.9 µm/m-°C
@Temperature 0.000 - 100 °C
8.28 µin/in-°F
@Temperature 32.0 - 212 °F
 16.7 µm/m-°C
@Temperature 0.000 - 315 °C
9.28 µin/in-°F
@Temperature 32.0 - 599 °F
 17.3 µm/m-°C
@Temperature 0.000 - 540 °C
9.61 µin/in-°F
@Temperature 32.0 - 1000 °F
 18.0 µm/m-°C
@Temperature 0.000 - 650 °C
10.0 µin/in-°F
@Temperature 32.0 - 1200 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity 15.6 W/m-K
@Temperature 0.000 - 100 °C
108 BTU-in/hr-ft²-°F
@Temperature 32.0 - 212 °F
Melting Point 1400 - 1455 °C2550 - 2651 °F
Solidus 1400 °C2550 °F
Liquidus 1455 °C2651 °F
Maximum Service Temperature, Air 980 °C1800 °FIntermittent
 1095 °C2003 °FContinuous Service
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.20 %<= 0.20 %
Chromium, Cr 23 %23 %
Iron, Fe 60 %60 %
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 14 %14 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
310 Stainless Steel, annealed plate
317 Stainless Steel, annealed plate
Outokumpu 253MA® High Temperature Austenitic Stainless Steel
304 Stainless Steel (UNS S30400); Annealed Plate
309 Stainless Steel, annealed, sheet

MQ309C / 12710

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.