MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Rogers Corporation RT/duroid® 6202PR High Frequency Laminate
Categories: Polymer

Material Notes: Features:
  • Low loss for excellent high frequency performance
  • Tight dielectric constant and thickness control
  • Excellent electrical and mechanical properties
  • Extremely low thermal coefficient of dielectric constant
  • In-plane expansion coefficient matched to copper
  • Very low etch shrinkage
  • Copper Cladding - Electrodeposited foil, Resistive foils, Rolled
  • Lead-free process compatible

Typical Applications:

  • Phase Array Antennas
  • Ground Based and Airborne Radar Systems
  • Global Positioning System Antennas
  • Power Backplanes
  • High Reliability Complex Multilayer Circuits
  • Commercial Airline Collision Avoidance Systems
  • Beam Forming Networks

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.10 g/cc0.0759 lb/in³ASTM D792
Moisture Absorption at Equilibrium 0.10 %0.10 %D24/23; IPC-TM-650 2.6.2.1
Thickness 127 - 762 microns5.00 - 30.0 milRange of Standard Thicknesses
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 30.0 MPa4350 psiX, Y direction; ASTM D638
Elongation at Break 4.9 %4.9 %X, Y direction; ASTM D638
Tensile Modulus 1.01 GPa146 ksiX, Y direction; ASTM D638
Compressive Modulus 1.035 GPa150.1 ksiZ direction; ASTM D638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmCondition A; Z direction; ASTM D257
Surface Resistance 1.00e+15 ohm1.00e+15 ohmCondition A; Z direction; ASTM D257
Dielectric Constant  2.86 - 2.94
@Thickness 0.127 mm,
Frequency 1e+10 Hz
2.86 - 2.94
@Thickness 0.00500 in,
Frequency 1e+10 Hz
Z direction; IPC-TM-650 2.5.5.5
 2.86 - 2.94
@Thickness 0.508 mm,
Frequency 1e+10 Hz
2.86 - 2.94
@Thickness 0.0200 in,
Frequency 1e+10 Hz
Z direction; IPC-TM-650 2.5.5.5
 2.94 - 3.02
@Thickness 0.254 mm,
Frequency 1e+10 Hz
2.94 - 3.02
@Thickness 0.0100 in,
Frequency 1e+10 Hz
Z direction; IPC-TM-650 2.5.5.5
 2.96 - 3.04
@Thickness 0.762 mm,
Frequency 1e+10 Hz
2.96 - 3.04
@Thickness 0.0300 in,
Frequency 1e+10 Hz
Z direction; IPC-TM-650 2.5.5.5
Dissipation Factor 0.0020
@Frequency 1e+10 Hz
0.0020
@Frequency 1e+10 Hz
Z direction; IPC-TM-650 2.5.5.5
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.0 µm/m-°C8.33 µin/in-°FX-Direction; 10°C/min; ASTM D3386; IPC-TM-650 2.4.41
 15.0 µm/m-°C8.33 µin/in-°FY-Direction; 10°C/min; ASTM D3386; IPC-TM-650 2.4.41
 30.0 µm/m-°C16.7 µin/in-°FZ-Direction; 10°C/min; ASTM D3386; IPC-TM-650 2.4.41
Specific Heat Capacity 0.930 J/g-°C0.222 BTU/lb-°Fcalculated
Thermal Conductivity 0.680 W/m-K
@Temperature 80.0 °C
4.72 BTU-in/hr-ft²-°F
@Temperature 176 °F
ASTM C518
Decomposition Temperature 500 °C932 °FTGA; ASTM D3850
Flammability, UL94 V-0V-0
 
Descriptive Properties
Thermal Coefficient of Dielectric Constant13 ppm/°CPreliminary; IPC-TM-650 2.5.5.5; 10 GHz; 0°C to 100°C; Z-Direction

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Corporation RO3003 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
Rogers Corporation RT/duroid® 6202 High Frequency Laminate
Rogers Corporation RO4533 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate
Rogers Corporation RO4450B Prepreg
Rogers Corporation RO4350B Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil

PROGA977 / 138417

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.