MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics WDS® Protection G-Plus Porextherm
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: WDS® Protection G-Plus is a 2-compound, inorganic coating which consists of layered silicates, water and inorganic binders in addition to a organic additive (<5%). WDS® Protection G-Plus can also be used as a coating for all WDS® products. The coating can be applied by spraying (recommended) or painting. The coating can be hardened at room temperature, although a hardening in an oven or drying oven at 80 - 120°C (176 - 212°F) is recommended for a optimum performance. WDS® Protection G-Plus is non-combustible and can be used up to a temperature of 1100°C (2012°F) after application. WDS® products which have a WDS® Protection G – Plus coating can be cut, drilled or milled without problems.

Information provided by Morgan Advanced Materials

Key Words: Porextherm
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 6.0after 48 hours; ConeSIMEX8
 9.0after 24 hours; ConeSIMEX8
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Cl (Chloride) 75 ppmASTM F 1277-02
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air <= 1100 °C
 
Descriptive Properties
Colorlight brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay EF5313 Polysiloxane Polymer
Solvay EF2000 Organosilicate Polymer
Morgan Advanced Ceramics Vacupor® NT-B-S Porextherm
Morgan Advanced Ceramics Unikote® Coating M Coating
Morgan Advanced Ceramics Firebrick SR 90 Thermal Ceramic

CMORF6114 / 202898

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.