MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SYNTHOS Kralex® 1739 Styrene Butadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: KRALEX® 1739 is a Specific grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 40% of chemically bounded styrene. It is coagulated by a system of acid and organic coagulant, contains 27% (37 PHR) of extender oil with reduced content of polycyclic aromatics (TDAE grade) and is stabilized by a staining antioxidant.

It is appropriate for rubber compounds used in the production of car tires and inner tubes, including tire re-trading, conveyor belts and various technical rubber articles.
KRALEX® 1739 can be used in the same rubber compounds as KRALEX® 1721 if the presence of polycyclic aromatics is not desirable.
It is not approved for production of rubber articles coming into contact with foods or drinking water.

Synthos was formerly known as Kaucuk. All information provided by Synthos.

Key Words: SBR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.75 %ASTM D5668
Mooney Viscosity 42 - 52
@Temperature 100 °C
(15-1.5 min); ASTM D3346
 50 - 60
@Temperature 100 °C
(1+4); ASTM D1646
Ash <= 0.40 %ASTM D5667
 
Chemical PropertiesOriginal ValueComments
Acid Value 4.1 - 5.7ASTM D5774
Styrene Content 40 %ASTM D5775
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 18.5 MPa35'/145°C; ASTM D412
Elongation at Break 370 %35'/145°C; ASTM D412
300% Modulus 0.0120 - 0.0180 GPa
@Strain 300 %
35'/145°C; ASTM D412
 
Descriptive Properties
50% of Vulcanization t' 50 (min.)6-10ASTM D5289
Antioxidant GradeStaining
Compound Safety ts 1 (min.)2.5-4.5ASTM D5289
Ethanol-toluene Extract (%)29-35ASTM D5774
Extender Oil Content (%)25-29
Extender Oil GradeTDAE
Maximal Moment (dNm)15-18ASTM D5289
Minimal Moment (dNm)1.8-2.6ASTM D5289
Optimal Vulcanization t' 90 (min.)11-16ASTM D5289
Soaps content (%)<= 0.3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dynasol Calprene® 1204B Solution Random SBR
Dow Buna® SB 1739 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Armacell Monarch® F-05091 (Black) Neoprene, EPDM, SBR Blend Foam
Rubatex R427 Neoprene/EPDM/SBR Rubber Foam Sheet
Monmouth Rubber & Plastics Superbounce 90 NEO/SBR

PSYNT011 / 82624

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.