MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dynasol Calprene® 1204B Solution Random SBR
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Calprene 1204B is a 75/25 Butadiene/Styrene Copolymer, polymerized in solution. It has a random structure with a typical vinyl content of 30%. It is presented in bales wrapped in low melting point polyethylene film.

Applications:

  • Tires
  • Footwear
  • Mechanical rubber goods

Compound Test Recipe: ISO-2322 (A)

Information provided by Dynasol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 120120Compounded, ML 1+4; ASTM D1646
 55
@Temperature 100 °C
55
@Temperature 212 °F
ML 1+4; ASTM D1646
Ash <= 0.20 %<= 0.20 %ASTM D5667
Collected Volatile Condensable Material 0.70 %0.70 %ASTM D5668
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 23.0 MPa3340 psiCompounded, 35 mins.; ISO 37
Elongation at Break 500 %500 %Compounded, 35 mins.; ISO 37
300% Modulus 15.0 MPa
@Strain 300 %
2180 psi
@Strain 300 %
Compounded, 35 mins.; ISO 37
 
Descriptive Properties
Hunterlab Color3ASTM D1925-70
Total Styrene (on polymer)25 %ASTM D5775

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Synthos BUNA™ cis 132 Schkopau High-cis Polybutadiene Rubber (PBR)
Dynasol Calprene® 375 Solution Random SBR
Dow SE BR-1220L Stereospecific high cis-1,4 Polybutadiene (BR)
Dow SE BR-1220M Stereospecific high cis-1,4 Polybutadiene (BR)
Dynasol Solprene® 375 Solution Random SBR

PDYNA12 / 34760

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.