System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Evonik VESTAMID® LX9012 PA 12
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 12 (PA12)
Material Notes:
Characterization: high viscosity, heat and light stabilized
Applications: transparent sport shoe soles, ski cover films
Information provided by Evonik
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.01
g/cc
ISO 1183
Moisture Absorption at Equilibrium
0.80 %
50% RH; ISO 62
Water Absorption at Saturation
1.5 %
ISO 62
Linear Mold Shrinkage, Flow
0.010
cm/cm
ISO 294-4
Linear Mold Shrinkage, Transverse
0.014
cm/cm
ISO 294-4
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
46.0
MPa
ISO 527-1/-2
Tensile Strength, Yield
37.0
MPa
ISO 527-1/-2
Elongation at Break
>= 50 %
ISO 527-1/-2
Elongation at Yield
5.0 %
ISO 527-1/-2
Tensile Modulus
1100
MPa
ISO 527
Charpy Impact Unnotched
NB
@Temperature 23.0 °C
ISO 179/1eU
NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched
13.0
kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
13.0
kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+14
ohm-cm
IEC 60093
Dielectric Constant
3.0
@Frequency 1e+6 Hz
ISO 60250
3.8
@Frequency 100 Hz
ISO 60250
Dielectric Strength
24.0
kV/mm
K20/P50; IEC 60423-1
Dissipation Factor
0.028
@Frequency 1e+6 Hz
IEC 60250
0.053
@Frequency 100 Hz
IEC 60250
Thermal Properties
Original Value
Comments
CTE, linear
130
µin/in-°F
@Temperature 23.0 - 55.0 °C
ISO 11359
Melting Point
176
°C
ISO 11357
Deflection Temperature at 0.46 MPa (66 psi)
120
°C
ISO 75
Deflection Temperature at 1.8 MPa (264 psi)
45.0
°C
ISO 75
Vicat Softening Point
130
°C
@Load 5.10 kg
Method B; ISO 306
170
°C
@Load 1.02 kg
Method A; ISO 306
Flammability, UL94
HB
@Thickness 1.60 mm
IEC 60695
HB
@Thickness 3.20 mm
IEC 60695
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Evonik VESTAMID® LX9008 PA 12
Arkema Platamid® H 005 Pellets Polyamide
Epsan Eplamid 66 GX0 25 KRMT Q1C5B502 Polyamide 66, Halogen Free
Evonik VESTAMID® LX9102 PA 12
Evonik VESTAMID® NRG 1001 PA 12
PEVONIL288 / 196492
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.