MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epsan Eplamid 66 GX0 25 KRMT Q1C5B502 Polyamide 66, Halogen Free
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Flame retardant polyamide 66 reinforced with 25% of glass fiber, heat stabilized for injection molding. Red phosphorous based, halogen free flame retardant grade, compliance with RoHs derivatives, with rating UL94 V0 and glow-wire at 960°C. It gives very good performance and high electrical demanding application.

Information provided by Epsan Plastik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ISO 1183
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inParallel; ISO 294-4
 0.0050 cm/cm0.0050 in/inNormal; ISO 294-4
Ash 25 %25 %ISO 3451-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress 150 MPa21800 psiISO 527-2
Elongation at Break 2.0 %2.0 %ISO 527-2
Tensile Modulus 9.40 GPa1360 ksiISO 527-2
Flexural Strength 245 MPa35500 psiISO 178
Flexural Modulus 8.70 GPa1260 ksiISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 550 V550 VEN 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 245 °C473 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °FISO 75-2/A
Vicat Softening Point 250 °C482 °FISO 306/B50
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
EN 60695-11-10
Glow Wire Ignition Temperature 750 °C
@Thickness 0.800 mm
1380 °F
@Thickness 0.0315 in
EN 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
EN 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 280 °C536 °FRecommended Injection Molding Temperature
Drying Temperature 80.0 °C176 °FAverage Drying Time is 2-4 hrs
Moisture Content 0.20 %0.20 %ISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo Technyl® A 60G1 V25 25% Glass Reinforced Nylon 66, Flame Retardant
Evonik VESTAMID® LX9012 PA 12
Domo TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY
BASF Ultramid® 66 H2 G/25-V0KB1 BK 3324 PA66 (Dry)
Envalior Akulon® SG-KGS6 PA66-GF30 FR

PEPSAN058 / 186372

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.