Description: Ultramid 66 H2 G/25-V0KB1 BK3324 is a 25% glass reinforced, heat stabilized injection molding grade. It's a V-0 self-extinguishing, with phosphorous. It offers good flowability, surface finish and good mechanical properties. It has excellent electrical properties.Information provided by BASF |