wire > 3.18 mm diameter gage length is 4 times diameter, wire < 3.18 mm gage length is 254 mm |
UNS S42000, AMS 5506, AMS 5621, ASTM A276, ASTM A314, ASTM A473, ASTM A580, FED QQ-S-763, FED QQ-S-766, FED QQ-W-423, MIL SPEC MIL-S-862, SAE J405 (51420), B.S. 420 S 37, B.S. CDS-18 (U.K), martensitic, DIN 1.4021, AFNOR Z 20 C 13 (Fr), UNI X 20 Cr 13, JIS SUS 420 J1, SS14 2303 (Sweden), ISO 683/13 4 |