MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elix Polymers Elix™ PC/5120 PC/ABS Polymer
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PC/ABS blend, injection molding grade with excellent mechanical properties balance up to -40°C. High flow, low emission grade , UV stabilized grade, good stability even with high humidity conditions, low shrinkage, good paintability, thin walled parts. Physical form: white to slightly yellowish pellets.

Property data measured at 23°C and 50% RH.

Information provided by Elix Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccISO 1183-1
Volatile Organic Compounds (VOC) Content <= 10 g/lVDA 278
Moisture Absorption at Equilibrium 0.20 %50% RH; ISO 62
Water Absorption at Saturation 0.70 %ISO 62
Linear Mold Shrinkage, Flow 0.0065 - 0.0075 cm/cm
@Thickness 2.00 mm
60 X 60 mm; ISO-294-4
Linear Mold Shrinkage, Transverse 0.0065 - 0.0075 cm/cm
@Thickness 2.00 mm
60 X 60 mm; ISO-294-4
Melt Flow 21 g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm³/10 min MVR; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 50.0 MPa50 mm/min; ISO 527-1,2
Elongation at Break >= 28 %50 mm/min; ISO 527-1,2
Tensile Modulus 2320 MPa1mm/min.; ISO 527-1,2
Flexural Strength 85.0 MPa2mm/min; ISO 178
Flexural Modulus 2320 MPa2mm/min; ISO 178
Izod Impact, Notched (ISO) 29.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
 30.0 kJ/m²
@Temperature -40.0 °C
ISO 180-1A
 51.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,2
CTE, linear, Transverse to Flow 82.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,2
Deflection Temperature at 0.46 MPa (66 psi) 120 °CISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 101 °CISO 75-1,2
Vicat Softening Point 118 °CB50, 50°C/h; ISO 306
 120 °CB120, 120°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
Flammability Test >= 80
@Thickness 1.00 mm
US-FMVSS , mm/min; ISO 3795
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °Cinjection molding; ISO 294
Mold Temperature 80.0 °Cinjection molding; ISO 294
Injection Velocity 240 mm/secinjection molding; ISO 294
 
Descriptive Properties
FOG Total Emission<10 µg/g23°C, VDA 278
Total Carbon Emission<15 µgC/g23°C, VDA 277

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® NH-1015 PC/ABS, Unreinforced FR
Lotte Advanced Materials Infino® PCA-NH1015V Flame Retardant
Covestro Bayblend® FR3000 PC/ABS Blend
Covestro Bayblend® FR 90 Polycarbonate + ABS Blend, Flame-Retardant
Elix Polymers Elix™ PC/5130 PC/ABS Polymer

PELIX927 / 192521

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.