System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Covestro Bayblend® FR 90 Polycarbonate + ABS Blend, Flame-Retardant
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Polycarbonate/ABS Alloy, Unreinforced
;
Polycarbonate (PC)
Material Notes:
Information provided by Bayer Corporation, Plastics Division
As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.17
g/cc
0.0423
lb/in³
ASTM D792
Linear Mold Shrinkage
0.0040
-
0.0060
cm/cm
0.0040
-
0.0060
in/in
ASTM D955
Spiral Flow
71.0
cm
@Thickness 2.50 mm
28.0
in
@Thickness 0.0984 in
at 254°C melt temp.
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
121
121
ASTM D785
Tensile Strength, Ultimate
45.0
MPa
6530
psi
ASTM D638
Tensile Strength, Yield
60.0
MPa
8700
psi
ASTM D638
Elongation at Break
70 %
70 %
ASTM D638
Elongation at Yield
4.0 %
4.0 %
ASTM D638
Tensile Modulus
2.80
GPa
406
ksi
ASTM D638
Flexural Yield Strength
100
MPa
14500
psi
at 5% strain; ASTM D790
Flexural Modulus
2.80
GPa
406
ksi
ASTM D790
Izod Impact, Notched
5.30
J/cm
@Thickness 3.17 mm
9.93
ft-lb/in
@Thickness 0.125 in
ASTM D256
Impact Test
57.0
J
@Thickness 3.20 mm
42.0
ft-lb
@Thickness 0.126 in
Instrumented Total Impact; 3.2 mm thick, 12.5 mm dart, 75 mm clamp, 6.7 m/s; ASTM D3763
Electrical Properties
Metric
English
Comments
Electrical Resistivity
1.00e+16
ohm-cm
1.00e+16
ohm-cm
IEC 112
Surface Resistance
1.00e+14
ohm
1.00e+14
ohm
IEC 93
Dielectric Constant
2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
ASTM D150
3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
IEC 250
Dielectric Strength
29.9
kV/mm
759
kV/in
IEC 243
Dissipation Factor
0.0050
@Frequency 100 Hz
0.0050
@Frequency 100 Hz
IEC 250
0.0070
@Frequency 1e+6 Hz
0.0070
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance
60
-
120
sec
@Thickness 3.00 mm
60
-
120
sec
@Thickness 0.118 in
UL Rating PLC 6 (60-120 sec)
Comparative Tracking Index
300
V
300
V
IEC 112
Hot Wire Ignition, HWI
60
-
120
sec
@Thickness 3.00 mm
60
-
120
sec
@Thickness 0.118 in
UL Rating PLC 1 (60-120 sec)
High Amp Arc Ignition, HAI
>=
120
arcs
@Thickness 1.50 mm
>=
120
arcs
@Thickness 0.0591 in
UL Rating PLC 0 (>120 arcs)
High Voltage Arc-Tracking Rate, HVTR
>=
150
mm/min
@Thickness 3.00 mm
>=
5.91
in/min
@Thickness 0.118 in
UL Rating PLC 4 (>150 mm/min.)
Thermal Properties
Metric
English
Comments
CTE, linear
77.0
µm/m-°C
@Temperature 20.0 °C
42.8
µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)
82.0
°C
@Thickness 6.35 mm
180
°F
@Thickness 0.250 in
Unannealed; ASTM D648
Vicat Softening Point
91.0
°C
196
°F
Rate B/120; ASTM D1525
UL RTI, Electrical
85.0
°C
@Thickness 1.57 mm
185
°F
@Thickness 0.0618 in
UL RTI, Mechanical with Impact
75.0
°C
@Thickness 1.57 mm
167
°F
@Thickness 0.0618 in
UL RTI, Mechanical without Impact
80.0
°C
@Thickness 1.57 mm
176
°F
@Thickness 0.0618 in
Flammability, UL94
V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Oxygen Index
30 %
30 %
ASTM D2836
Processing Properties
Metric
English
Comments
Melt Temperature
220
-
270
°C
428
-
518
°F
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Elix Polymers Elix™ PC/5120 PC/ABS Polymer
Lotte Advanced Materials Infino® NH-1015 PC/ABS, Unreinforced FR
Covestro Bayblend® FR 90 Polycarbonate/ABS Blend
Covestro Makrolon® FR 6002 Polycarbonate
Celanese Zytel® 70G30L NC010 PA66-GF30
PB1B08 / 26401
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.