  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Mineral Fiber Paper 400-LS Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Mineral Fiber, Utility grade fiber. 400-LS paper is produced from premium, high quality mineral fibers and organic binders in a unique paper making process. This utility grade paper is noted for good tensile strengths, outstanding handling characteristics, and good insulating values, while being very cost effective. The 400-LS product is a very clean, low shot paper with a high quality surface texture and low thermal conductivity value. 400-LS paper can be die-cut in accordance with customer specifications in a variety of shapes and sizes.

Applications:

  • High temperature gasketing
  • Automotive heat shields and muffler insulation
  • Ladle refractory back up
  • Glass tank refractory back up
  • Appliance/radiant heater insulation
  • Back up for aluminum troughs and metal transfer parts
  • Back up lining for aluminum holding furnaces.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.192 - 0.240 g/cc
Loss On Ignition 5.0 - 10 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 0.306 - 0.714 kg(f)/cm²fired
 2.86 - 5.30 kg(f)/cm²
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0500 W/m-K
@Temperature 260 °C
ASTM C201
 0.0800 W/m-K
@Temperature 538 °C
ASTM C201
 0.110 W/m-K
@Temperature 704 °C
ASTM C201
Melting Point 1093 °C
Maximum Service Temperature, Air <= 732 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 15 %
CaO 21 %
Other 22 %
SiO2 43 %
 
Descriptive Properties
Classification Temperature (°C)816
Coloroff-white
Fiber Index (%)70

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Ceramic Fiber Board S Board Ceramic Fibre Board
Thermal Ceramics Alfibond 2100 Shapes
Morgan Advanced Ceramics Ceramic Fiber Ropes Twisted Ceramic Fiber
Morgan Advanced Ceramics Ceramic Fiber Blankets Cerawool Blanket
Morgan Advanced Ceramics Ceraform 250 Ceramic Fiber

CMORF6430 / 203214

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.