MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Alathon® M6080WC High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Applications
ALATHON M 6080WC is a natural, high density, polyethylene homopolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control cable applications including gas-injected or chemically expanded insulation. This resin provides enhanced processability and stiffness and exhibits excellent color, low odor and good processing stability.

Processing Techniques
M 6080WC, like other thermoplastic polyolefin resins, can be extruded as wire and cable insulation using a conventional extruder. Below are suggested extrusion conditions for M 6080WC. These conditions are intended as general guidelines only and are not optimum values, since manufacturing conditions such as extruder type and size affect the processing of thermoplastic resins.

This product is from the former Equistar product line.

Key Words: HDPE; Fiber Optic/Coaxial; Insulation
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.958 g/ccASTM D1505
Melt Flow 8.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 67ASTM D2240
Tensile Strength at Break 3100 psiASTM D638
Tensile Strength, Yield 3900 psiASTM D638
Elongation at Break 1900 %ASTM D638
Flexural Modulus, 1% Secant 192000 psiASTM D790
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 3.00e+17 ohm-cmASTM D257
Dielectric Constant 2.36
@Frequency 1e+6 Hz
ASTM D1531
Dielectric Strength 700 V/milDC; ASTM D149
Dissipation Factor 0.000030
@Frequency 1e+6 Hz
ASTM D1531
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 130 °CASTM D1525
Brittleness Temperature <= -76.0 °CF50; ASTM D746
 
Processing PropertiesOriginal ValueComments
Feed Temperature 300 - 325 °F
Zone 2 350 - 400 °F
Zone 3 400 - 450 °F
Zone 4-x 475 - 500 °F
Adapter Temperature 475 - 500 °F
Die Temperature 475 - 500 °F
Melt Temperature 475 - 500 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Alathon® M5370WC High Density Polyethylene
LyondellBasell Petrothene® LR590005 High Density Polyethylene
Borealis HE3366 High Density Polyethylene
LyondellBasell Petrothene® LR590001 High Density Polyethylene
Borealis HE4872 High Density Polyethylene

PEQU0266 / 36700

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.