MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis HE3366 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: HE3366 is a HDPE compound for solid insulation of telephone singles with high extrusion speed. HE3366 is designed as insulation for petroleum filled telephone cables. It is also suitable as outer skin in "foam-skin" constructions. Specifications: ISO 1872-PE; KGHN; 45-D006; ASTM D1248 Type III, Class A, Category 4, Grade E8, E9; the following cable material standards: EN 50290-2-23; DIN VDE 0207, 2YI1; IEC 60708; EN 50407; and DIN VDE 0818.

Information provided by Borealis AG

Key Words: HDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.945 g/cc0.0341 lb/in³ISO 1183/ISO 1872-2
ESCR 10% Igepal® >= 48 hour
@Temperature 50.0 °C
>= 48 hour
@Temperature 122 °F
F20; IEC 60811-4-1/B
Oxidative Induction Time (OIT) 50 min
@Temperature 200 °C
50 min
@Temperature 392 °F
IEC 60811-4-2/B
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 61611s; ISO 868
Tensile Strength at Break 23.0 MPa3340 psiISO 527
Elongation at Break 600 %600 %ISO 527-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+6 ohm-cm1.00e+6 ohm-cmIEC 60093
Dielectric Constant 2.33
@Frequency 1e+6 Hz
2.33
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 22.0 kV/mm559 kV/inIEC 60243
Dissipation Factor 0.000060
@Frequency 1e+6 Hz
0.000060
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 100 - 120 °C212 - 248 °Fconductor preheating temperature
Melt Temperature 220 - 250 °C428 - 482 °F
Die Cooling Temperature 50.0 °C122 °Fwater cooling
 
Descriptive Properties
Petroleum Jelly Absorption (%)5IEC 60811-4-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis HE4872 High Density Polyethylene
BASF Novolen® 2700 L Polypropylene
BASF Novolen® 3300 MC Polypropylene
LyondellBasell Alathon® M5370WC High Density Polyethylene
LyondellBasell Alathon® M6080WC High Density Polyethylene

PBOREA482 / 108741

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.