MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik 12.LNb Welding wire
Categories: Metal; Ferrous Metal; Ferritic

Material Notes: Sandvik 12.LNb is a filler metal giving a ferritic micro structure. The niobium addition forms carbides to improve corrosion resistance, increase strength at higher temperatures, and promote the ferritic micro structure. Sandvik 12.LNb may be used to join matching or dissimilar base metals. The greatest usage is for applications where thin stock is fabricated into exhaust system components.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 450 MPa
Elongation at Break 20 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.040 %AIM
 <= 0.040 %All-Weld Metal
Chromium, Cr 11.3 %AIM
 11.3 %All-Weld Metal
Manganese, Mn 0.40 %All-Weld Metal
 0.60 %AIM
Niobium, Nb (Columbium, Cb) 0.50 %AIM
 0.50 %All-Weld Metal
Phosphorus, P <= 0.030 %AIM
 <= 0.030 %All-Weld Metal
Silicon, Si 0.50 %All-Weld Metal
 0.60 %AIM
Sulfur, S <= 0.015 %AIM
 <= 0.015 %All-Weld Metal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV5067 / 199631

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.