Sandvik 12.LNb is a filler metal giving a ferritic micro structure. The niobium addition forms carbides to improve corrosion resistance, increase strength at higher temperatures, and promote the ferritic micro structure. Sandvik 12.LNb may be used to join matching or dissimilar base metals. The greatest usage is for applications where thin stock is fabricated into exhaust system components.Information provided by Sandvik |