MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Overview of materials for Polypropylene, Glass/Mineral Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Glass/Mineral Reinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.910 - 1.63 g/ccAverage value: 1.16 g/cc Grade Count:157
Filler Content 10.0 - 40.0 %Average value: 27.1 % Grade Count:37
Water Absorption 0.0100 - 0.300 %Average value: 0.0541 % Grade Count:37
Linear Mold Shrinkage 0.00100 - 0.0150 cm/cmAverage value: 0.00459 cm/cm Grade Count:126
 0.00200 - 0.00200 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00200 cm/cm Grade Count:1
Linear Mold Shrinkage, Transverse 0.00400 - 0.0120 cm/cmAverage value: 0.00651 cm/cm Grade Count:15
 0.00500 - 0.00500 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00500 cm/cm Grade Count:1
Melt Flow 1.00 - 34.5 g/10 minAverage value: 8.25 g/10 min Grade Count:116
Ash 28.0 - 40.0 %Average value: 31.1 % Grade Count:31
 30.0 - 30.0 %
@Temperature 625 - 625 °C
Average value: 30.0 % Grade Count:1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 53.0 - 70.0Average value: 64.0 Grade Count:3
Hardness, Rockwell R 40.0 - 117Average value: 89.1 Grade Count:55
Hardness, Shore D 73.0 - 80.0Average value: 75.7 Grade Count:15
Tensile Strength, Ultimate 20.0 - 150 MPaAverage value: 53.3 MPa Grade Count:112
 9.00 - 80.0 MPa
@Temperature 60.0 - 120 °C
Average value: 31.0 MPa Grade Count:2
Tensile Strength, Yield 20.0 - 85.0 MPaAverage value: 51.1 MPa Grade Count:70
Elongation at Break 1.00 - 100 %Average value: 7.09 % Grade Count:95
 2.90 - 2.90 %
@Temperature 80.0 - 80.0 °C
Average value: 2.90 % Grade Count:1
Elongation at Yield 3.00 - 100 %Average value: 7.99 % Grade Count:35
Modulus of Elasticity 1.90 - 12.3 GPaAverage value: 5.03 GPa Grade Count:58
 8.80 - 8.80 GPa
@Temperature 80.0 - 80.0 °C
Average value: 8.80 GPa Grade Count:1
Flexural Yield Strength 31.0 - 220 MPaAverage value: 82.5 MPa Grade Count:103
 120 - 120 MPa
@Temperature 80.0 - 80.0 °C
Average value: 120 MPa Grade Count:1
Flexural Modulus 1.44 - 11.4 GPaAverage value: 4.54 GPa Grade Count:155
 0.600 - 7.80 GPa
@Temperature 60.0 - 120 °C
Average value: 3.05 GPa Grade Count:2
Compressive Yield Strength 39.3 - 62.1 MPaAverage value: 50.7 MPa Grade Count:7
Izod Impact, Notched 0.250 - 6.00 J/cmAverage value: 0.739 J/cm Grade Count:123
 0.250 - 2.00 J/cm
@Temperature -40.0 - 0.000 °C
Average value: 1.08 J/cm Grade Count:4
 2.1356 - 2.1356 J/cm
@Temperature -28.9 - -28.9 °C
Average value: 1.08 J/cm Grade Count:1
 2.1356 - 2.1356 J/cm
@Thickness 3.17 - 3.17 mm
Average value: 1.08 J/cm Grade Count:1
Izod Impact, Unnotched 1.60 - 7.47 J/cmAverage value: 3.76 J/cm Grade Count:34
Izod Impact, Notched (ISO) 3.00 - 25.0 kJ/m²Average value: 7.37 kJ/m² Grade Count:15
 3.70 - 18.0 kJ/m²
@Temperature -40.0 - 0.000 °C
Average value: 6.63 kJ/m² Grade Count:6
Charpy Impact Unnotched 1.80 - 1000 J/cm²Average value: 3.81 J/cm² Grade Count:17
 1.00 - 7.20 J/cm²
@Temperature -40.0 - 0.000 °C
Average value: 3.59 J/cm² Grade Count:8
Charpy Impact, Notched 0.220 - 3.70 J/cm²Average value: 0.941 J/cm² Grade Count:24
 0.130 - 3.90 J/cm²
@Temperature -40.0 - 0.000 °C
Average value: 0.915 J/cm² Grade Count:13
Gardner Impact 0.339 - 5.42 JAverage value: 0.880 J Grade Count:24
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 - 1.00e+17 ohm-cmAverage value: 2.80e+16 ohm-cm Grade Count:17
Surface Resistance 1.00e+14 - 1.00e+15 ohmAverage value: 8.50e+14 ohm Grade Count:6
Dielectric Constant 2.30 - 3.50Average value: 2.78 Grade Count:17
Dielectric Strength 19.7 - 40.0 kV/mmAverage value: 23.6 kV/mm Grade Count:16
Dissipation Factor 0.00200 - 0.00600Average value: 0.00275 Grade Count:8
Arc Resistance 120 - 130 secAverage value: 125 sec Grade Count:11
Comparative Tracking Index 600 - 650 VAverage value: 615 V Grade Count:17
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.6 - 75.0 µm/m-°CAverage value: 44.4 µm/m-°C Grade Count:18
Thermal Conductivity 0.303 - 0.360 W/m-KAverage value: 0.336 W/m-K Grade Count:9
Melting Point 160 - 182 °CAverage value: 167 °C Grade Count:18
Hot Ball Pressure Test 125 °CAverage value: 125 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 96.1 - 169 °CAverage value: 150 °C Grade Count:112
Deflection Temperature at 1.8 MPa (264 psi) 35.6 - 155 °CAverage value: 126 °C Grade Count:128
Vicat Softening Point 55.0 - 160 °CAverage value: 124 °C Grade Count:25
Flammability, UL94 HB - V-0Grade Count:64
Oxygen Index 20.0 - 21.0 %Average value: 20.8 % Grade Count:4
Glow Wire Test 550 - 750 °CAverage value: 650 °C Grade Count:9
 
Processing PropertiesOriginal ValueComments
Processing Temperature 30.0 - 270 °CAverage value: 212 °C Grade Count:26
Nozzle Temperature 54.4 - 260 °CAverage value: 222 °C Grade Count:37
Melt Temperature 180 - 270 °CAverage value: 224 °C Grade Count:55
Mold Temperature 20.0 - 90.0 °CAverage value: 48.4 °C Grade Count:75
Drying Temperature 60.0 - 120 °CAverage value: 79.5 °C Grade Count:49
Moisture Content 0.0500 - 0.200 %Average value: 0.0619 % Grade Count:21
Injection Pressure 2.76 - 120 MPaAverage value: 52.5 MPa Grade Count:36

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Molded
Overview of materials for Polypropylene with 10% Glass Fiber Filler
Overview of materials for Polypropylene with 40% Glass Fiber Filler
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
Overview of materials for Polypropylene with 20% Glass Fiber Filler

O4738 / 78389

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.