Turco R 9100 GL is a viscous pink emulsion that does not contain any aromatic hydrocarbons, phosphates, borates, silicates or hydrogen peroxide. It was developed as a neutral pH product for removal of paint systems utilizing a polyamide type intermediate coating to allow for selective stripping of the topcoat layers while leaving the primer layer intact. Complies fully with the aircraft / aerospace NESHAP to minimize hazards in work areas. Safe on aircraft metals, including magnesium and high strength steel. Very low evaporative loss allows for extended dwell times and one stripping coat removal. |
Aerospace Surface Treatment |