MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Henkel Turco R 9100 GL Paint Remover
Categories: Fluid; Solvent

Material Notes: Turco R 9100 GL is a viscous pink emulsion that does not contain any aromatic hydrocarbons, phosphates, borates, silicates or hydrogen peroxide. It was developed as a neutral pH product for removal of paint systems utilizing a polyamide type intermediate coating to allow for selective stripping of the topcoat layers while leaving the primer layer intact. Complies fully with the aircraft / aerospace NESHAP to minimize hazards in work areas. Safe on aircraft metals, including magnesium and high strength steel. Very low evaporative loss allows for extended dwell times and one stripping coat removal.

Key Words: Aerospace Surface Treatment
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesMetricEnglishComments
Processing Temperature 23.0 °C73.4 °F
 
Descriptive Properties
ChemistryAlkaline
ConsistencyLiquid
FormReady-to-Use
SubstrateAluminum
 Composite Materials

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHENK963 / 146968

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.