MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond EP110F6 Thermal Shock Resistant, Electrically Insulating Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Master Bond Polymer System EP110F6 is a two component high performance epoxy resin system with a long pot life at room temperature which is specifically designed for potting, sealing, encapsulating and casting. It requires an elevated temperature cure. EP110F6 has good thermal shock resistance and thermal cycling properties along with excellent electrical insulation characteristics.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 15000 - 20000 cP
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 155 °F
Minimum Service Temperature, Air -55.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 1.50 hourAt 160°F plus 6-10 hrs at 300°F
 
Descriptive Properties
Color Code"A" Clear; "B" Amber
Mix Ratio by weight50/100
Set-Up Time, minutes720-1440At Room Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond MasterSil 151AO Thermally Conductive Silicone System
Master Bond MasterSil 151AN Silicone Features High Thermal Conductivity
Master Bond EP22 Two Component, Aluminum Filled, Epoxy System
Master Bond EP21AOLV-1 Two Part, Room Temperature Curing Epoxy System
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting

PMASTB069 / 52226

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.