MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP22 Two Component, Aluminum Filled, Epoxy System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Easily machinable
  • Two component epoxy
  • One to one mix ratio
  • Exceptionally high compressive strength
  • Superior dimensional stability
  • Aluminum filled
Product Description: Master Bond EP22 is an aluminum filled, two component epoxy adhesive for high performance bonding, sealing and coating. It is formulated to cure at room temperature or more rapidly at elevated temperatures, with a noncritical one to one mix ratio by weight or volume. EP22 is especially noteworthy for its sterling machinability, great dimensional stability and exceptionally high compressive strength. It bonds well to metals, especially steel and aluminum, as well as ceramics, composites, rubbers and many plastics. It has good void filling properties. The cured epoxy responds well to thermal cycling and has fine chemical resistance when exposed to water, fuels and oils. Although it is aluminum filled, it is a respectable electrical insulator. The presence of aluminum also promotes lower shrinkage than most epoxy systems. EP22 has an operating temperature range of -60°F to +250°F. The color of Part A is gray and Part B is gray. Master Bond EP22 system is widely used in specialty OEM, aerospace, chemical processing and selected electronic applications. It can be cured in thicker sections, and in this context it has utility as a cost effective repair and maintenance formulation for a wide range of machinery, especially industrial process equipment.

Product Advantages:

  • Convenient mixing: forgiving one to one mix ratio by weight or volume
  • Easy to apply — adhesive spreads evenly and smoothly; non-drip viscosity
  • Ambient temperature curing imparts optimal chemical resistance and hardness
  • Forms tough bonds; resistant to thermal cycling
  • Bonds well to a variety of substrates
  • Superb resistance to oils, fuels and related chemicals

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 70000 - 100000 cP70000 - 100000 cPPart A
 100000 - 150000 cP100000 - 150000 cPPart B
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 80>= 80
Tensile Strength >= 51.7 MPa>= 7500 psi
Compressive Strength >= 68.9 MPa>= 10000 psi
Adhesive Bond Strength >= 20.7 MPa>= 3000 psiTensile lap, Aluminum to Aluminum
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 7.5
@Frequency 60 Hz
7.5
@Frequency 60 Hz
Dielectric Strength >= 3.94 kV/mm
@Thickness 3.17 mm
>= 100 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 35.0 - 40.0 µm/m-°C19.4 - 22.2 µin/in-°F
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 93.3 °C
2.00 - 3.00 hour
@Temperature 200 °F
 2880 - 4320 min
@Temperature 23.9 °C
48.0 - 72.0 hour
@Temperature 75.0 °F
Working Life 90.0 - 120 min90.0 - 120 minAfter mixing, 100 g batch
Shelf Life 12.0 Month
@Temperature <=23.9 °C
12.0 Month
@Temperature <=75.0 °F
in original, unopened containers
 
Descriptive Properties
Mixing Ratio1:1 by weight or volumeParts A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond MasterSil 151AO Thermally Conductive Silicone System
Master Bond MasterSil 151AN Silicone Features High Thermal Conductivity
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting
Master Bond EP110F6 Thermal Shock Resistant, Electrically Insulating Epoxy
Cotronics Duralco™ 135 500°F (260°C) Aluminum Filled Epoxy

PMASTM844 / 185437

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.