MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Multibase TPSiV® 1180-50D Thermoplastic Silicone Vulcanizate  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV); Nylon (Polyamide PA); Silicone, Thermoplastic

Material Notes: TPV product based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced by dynamic “vulcanization” or cross-linking of silicone polymers within the thermoplastic organic phase and results in a stable droplet type morphology as shown in the TEM micrograph. TPSiV™ combines the elastomeric performance of silicone rubber with the melt re-processability and thermal and chemical resistance of engineering thermoplastics.

Nylon based TPSiV™ (1180-50D) has found use as the jacketing material in automotive brake cables due to its excellent temperature and chemical resistance.

Information provided by Multibase. Multibase is now a DuPont brand; this grade was discontinued prior to DuPont's acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 525210 sec; ASTM D2240
Tensile Strength at Break 24.0 MPa3480 psiASTM D412
Elongation at Break 200 %200 %ASTM D412
Tear Strength 24.5 kN/m140 pliASTM D412
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.044.04ASTM D150
Dielectric Strength 22.4 kV/mm569 kV/inASTM D149
 22.4 kV/mm
@Frequency 100 Hz
569 kV/in
@Frequency 100 Hz
ASTM D149
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 °C446 °F
Middle Barrel Temperature 240 °C464 °F
Front Barrel Temperature 250 °C482 °F
Nozzle Temperature 260 °C500 °F
Zone 1 210 °C410 °F
Zone 2 220 °C428 °F
Zone 3 220 °C428 °F
Zone 4 220 °C428 °F
Zone 5 220 °C428 °F
Die Temperature 230 °C446 °F
Melt Temperature 235 °C455 °F
Mold Temperature 10.0 - 30.0 °C50.0 - 86.0 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2 - 4 hour2 - 4 hour
 
Descriptive Properties
Injection RateFast

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Multibase TPSiV® 3011-70A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 4200-80A Thermoplastic Silicone Vulcanizate
Wacker Geniomer® 200 Silicone TPE Elastomer
Multibase TPSiV® 3040-60A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 3340-65A Thermoplastic Silicone Vulcanizate

PMULTI301 / 93491

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.