MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Multibase TPSiV® 1180-50D Thermoplastic Silicone Vulcanizate  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV); Nylon (Polyamide PA); Silicone, Thermoplastic

Material Notes: TPV product based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced by dynamic “vulcanization” or cross-linking of silicone polymers within the thermoplastic organic phase and results in a stable droplet type morphology as shown in the TEM micrograph. TPSiV™ combines the elastomeric performance of silicone rubber with the melt re-processability and thermal and chemical resistance of engineering thermoplastics.

Nylon based TPSiV™ (1180-50D) has found use as the jacketing material in automotive brake cables due to its excellent temperature and chemical resistance.

Information provided by Multibase. Multibase is now a DuPont brand; this grade was discontinued prior to DuPont's acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 5210 sec; ASTM D2240
Tensile Strength at Break 3480 psiASTM D412
Elongation at Break 200 %ASTM D412
Tear Strength 24.5 kN/mASTM D412
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.04ASTM D150
Dielectric Strength 569 V/milASTM D149
 569 V/mil
@Frequency 100 Hz
ASTM D149
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 446 °F
Middle Barrel Temperature 464 °F
Front Barrel Temperature 482 °F
Nozzle Temperature 500 °F
Zone 1 410 °F
Zone 2 428 °F
Zone 3 428 °F
Zone 4 428 °F
Zone 5 428 °F
Die Temperature 446 °F
Melt Temperature 455 °F
Mold Temperature 50.0 - 86.0 °F
Drying Temperature 176 °F
Dry Time 2 - 4 hour
 
Descriptive Properties
Injection RateFast

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Multibase TPSiV® 3011-70A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 4200-80A Thermoplastic Silicone Vulcanizate
Wacker Geniomer® 200 Silicone TPE Elastomer
Multibase TPSiV® 3040-60A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 3340-65A Thermoplastic Silicone Vulcanizate

PMULTI301 / 93491

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.