MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 Tacna® 2000 NLGI No. 1
Categories: Fluid; Lubricant; Lithium Gellant; Organic Soap Gellant

Material Notes: Description: Conoco Tacna 2000 is available in two NLGI grades: No. 1 and No. 2. The No. 2 grade is ideal for use in heavily loaded sleeve-type bushings and bearings subjected to shock loading and operated at medium to high ambient temperatures. It is also ideal for use as a fifth wheel grease commonly found on tractor/trailers. The No. 1 grade provides better fluidity and is recommended for lower ambient temperatures. Tacna 2000 is manufactured from high-viscosity index paraffinic base oils and lithium 12-hydroxy stearate soap stock. It is fortified with an adhesive polymer, rust and corrosion inhibitors, and an effective extreme-pressure additive, which results in an exceptionally stable grease that resists separation under heavy loads. It is also extremely resistant to water washing, as evidenced by its excellent water-washout and spray-off characteristics. Tacna 2000 contains an effective polymer which prevents oil bleeding while providing an exceptional level of protection under shock loading conditions.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 95Viscosity Index (Base Oil Property)
Saybolt Viscosity at 100°F 880 SUSBase Oil Property
Saybolt Viscosity at 210°F 86 SUSBase Oil Property
Kinematic Viscosity at 40°C (104°F) 140 cStBase Oil
Kinematic Viscosity at 100°C (212°F) 14 cStBase Oil
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 315 kg
Four Ball Wear 0.480 mm
Penetration 309 - 341Worked 10,000 strokes
Penetration P(60), 1/10 mm 325
Timken Test 45.0 lb
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 275 °F
Minimum Service Temperature, Air 0.000 °F
Pour Point 10.0 °F(Base Oil Property)
Dropping Point 400 °F
 
Descriptive Properties
ASTM Rust Test (A & B)Pass
ColorAmber
Copper Corrosion3A
Low Temperature Mobility0.2 gm/secat 0°F
 0.6 gm/secat 10°F
 0.8 gm/secat 20°F
Mobility0.16 g/s0°F
 0.19 g/s10°F
 0.27 g/s20°F
Oxidation Stability3 psi drop/100 hrs
 7 psi drop/500 hrs
Roll Stability5% Change
Soap Type (Thickener)Lithium
Water Spray Off11 wt.% Loss
Water Washout15 wt.% Loss175°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON228 / 75265

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.