Product Description: Regalite™ C6100L Hydrocarbon Resin is a hydrogenated water-white hydrocarbon resin developed derived from petrochemical feedstocks. This resin is especially designed as a component of a multipart tackifier system in hot melt and solvent based pressure sensitive adhesives based on SIS, SBS and SEBS thermoplastic block copolymers, providing superior tack, adhesion and cohesive strength characteristics. Application/Uses: - Adhesives
- Hot Melt Adhesives
- Pressure sensitive adhesives
- Tackifier
Key Attributes: - Excellent heat stability
- Water-white color
- Wide compatibility
Information provided by Eastman |