MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eastman Regalite™ C6100L Hydrocarbon Resin
Categories: Other Engineering Material

Material Notes: Product Description: Regalite™ C6100L Hydrocarbon Resin is a hydrogenated water-white hydrocarbon resin developed derived from petrochemical feedstocks. This resin is especially designed as a component of a multipart tackifier system in hot melt and solvent based pressure sensitive adhesives based on SIS, SBS and SEBS thermoplastic block copolymers, providing superior tack, adhesion and cohesive strength characteristics.

Application/Uses:

  • Adhesives
  • Hot Melt Adhesives
  • Pressure sensitive adhesives
  • Tackifier
Key Attributes:
  • Excellent heat stability
  • Water-white color
  • Wide compatibility

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 205 cP
@Temperature 180 °C
205 cP
@Temperature 356 °F
 
Thermal PropertiesMetricEnglishComments
Ring & Ball Softening Point 95.0 - 105 °C203 - 221 °FASTM E28
 
Optical PropertiesMetricEnglishComments
Yellow Index 6.0 - 13 %6.0 - 13 %2 cm cell; ASTM E313
Gardner Color Number <= 1.0<= 1.0ASTM D6166

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5543 / 222737

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.