MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond Supreme 18TC One Component Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Can be applied in very thin bond lines
  • High thermal conductivity
  • Excellent bonding strength
  • Unmatched heat transfer capabilities
Product Description: Master Bond Supreme 18TC is a cutting edge material pertaining to the thermal management of epoxies. This system utilizes a special blend of highly thermally conductive filler material that is capable of being applied in bond lines as thin as 10-15 microns. Supreme 18TC maintains high bond strength properties even when exposed to hostile environmental conditions, including elevated temperatures. Supreme 18TC has very low thermal resistance, since it is highly thermally conductive and able to cure effectively in thin layers. Another way of looking at this is to say that the lower the thermal resistance, the better the heat transfer. In this regard, Master Bond utilizes the principles based on the formula: R=t/K (where “R” is the thermal resistance; “t”, the thickness and “K” the thermal conductivity of the material). Using specific values, when standard alumina filled thermally conductive epoxy is applied in 50 micron thick sections, the thermal resistance is 30-35 x 10-6 K•m2/W. With Supreme 18TC, the thermal resistance is significantly lower: 5-7 x 10-6 K•m2/W, because of the filler and its ability to be effectively applied in sections of 10-15 microns in width. Simply put, this epoxy is second to none when transferring heat. Significantly, Supreme 18TC is a one part system that requires no mixing. Its working life is essentially unlimited as it is not premixed and frozen. It is has a smooth paste consistency that requires heat curing for 60-90 minutes at 250-300°F with a post cure of a few hours to obtain optimal properties. Some other positives include low shrinkage upon curing, a low CTE and a high degree of dimensional stability. It bonds well to a wide variety of substrates including metals, composites, ceramics and plastics. Supreme 18TC is designed to withstand thermal cycling and shock. Electrically, it is an outstanding insulator. The operating temperature is 4K to +400°F and the color is gray. The forte of Supreme 18TC is high heat transfer and its simple handling, which allows it to be a prime candidate for sophisticated, high-tech applications. Some of the industries where this can be used include aerospace, electronic, optical, specialty OEM and cryogenic industries.

Product Advantages:

  • One part system; no mixing required
  • Cures readily at 250-300°F with a post cure at 350°F
  • High thermal conductivity and electrical insulation values
  • Will cure effectively in very thin sections
  • Superior thermal cycling capabilities
  • Exceptionally low thermal resistance
  • Meets NASA low outgassing specifications

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80 - 90
Tensile Strength 6000 - 7000 psi
Compressive Strength 22000 - 24000 psi
Adhesive Bond Strength 2200 - 2400 psiTensile Lap, Aluminum to Aluminum
Peel Strength 5.00 - 10.0 plialuminum to aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 4.8
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 22.0 - 25.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -269 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 4.00 hour
@Temperature 177 °C
Recommended post cure
 60.0 - 90.0 min
@Temperature 121 - 149 °C
Shelf Life 3.00 - 6.00 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
Viscositysmooth paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond Supreme 42HT-2 Toughened Epoxy Resists Thermal Cycling
Master Bond EP48TC Two Part Epoxy Adhesive
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting
Master Bond EP30LTE-LO Dimensionally Stable Low Outgassing Two Part Epoxy
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy

PMASTM961 / 185554

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.