MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Styrolux® 656C SBC
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styrolux® 656C is a clear styrene-butadiene copolymer (SBC) with enhanced flow properties. It is used almost exclusively for injection molding of rigid, tough parts requiring highest levels of clarity and surface gloss. Styrolux® 656C is sterilizable by gamma-rays and offers good hinge properties. Tough and stiff grade, Enhanced flowability, High clarity. Applications: Molded containers and bottles, Toys, Displays, Appliance housings, Medical devices, Garment hangers

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Key Words: 656 C
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
Water Absorption at Saturation 0.070 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage 0.0030 - 0.010 cm/cmISO 294-4
Melt Flow 16 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 72ISO 868
Tensile Strength, Yield 35.0 MPaISO 527
Elongation at Break 20 %Nominal; ISO 527
 20 %ISO 527
Elongation at Yield 2.4 %ISO 527
Tensile Modulus 1800 MPaISO 527
Flexural Strength 48.0 MPaISO 178
Flexural Yield Strength 48.0 MPa
@Strain 5.0 %
Flexural Modulus 1900 MPaISO 178
Izod Impact, Notched 21.0 J/mASTM D256
Izod Impact, Notched (ISO) 2.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 3.00 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched 25.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 2.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 1550 MPaISO 899
Tensile Creep Modulus, 1000 hours 1050 MPaISO 899
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohmIEC 60093
Dielectric Constant 2.5IEC 60250
Dissipation Factor 0.00030
@Frequency 100 Hz
IEC 60250
 0.00080
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 - 90.0 µm/m-°CISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °Cannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °Cannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 63.0 °C
@Load 5.10 kg
VST/B/50. 50C/h; ISO 306
 85.0 °C
@Load 1.02 kg
VST/A/50. 50C/h; ISO 306
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.579Sodium D Line; ISO 489
Haze 1.5 %ASTM 1003
Transmission, Visible 90 %
@Wavelength 550 nm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 250 °CISO 294
Mold Temperature 30.0 - 50.0 °CISO 294
 
Descriptive Properties
ColorCrystal Clear
Commercial StatusEurope
Primary Processing TechniqueInjection Molding
Transparency0.9d=2mm, DIN 5036-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Lustran® SAN 31 Styrene Acrylonitrile (SAN)
Overview of materials for Styrene-Butadiene Copolymer, SBC
INEOS Styrolution PS 5600/5601 HIPS
INEOS Styrolution Terlux® 2802 Transparent MABS
Overview of materials for Polycarbonate, Molded

PBASG0638 / 132271

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.