MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboCast/AboCure 8109-3
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Low viscosity, RT cure. Easy processing.

Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140°F), 15 min/100°C (212°F).

Applications: Laminating, small parts, and potting.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³
Water Absorption 0.30 - 0.50 %0.30 - 0.50 %(60x10X4 mm bar) after 10 days at 20°C (77°F)
 0.70 - 1.0 %0.70 - 1.0 %(60x10X4 mm bar) after 1 hour at 100°C (212°F)
Viscosity 1600 - 2000 cP1600 - 2000 cP
Vapor Pressure  <= 0.0000133 bar
@Temperature 20.0 °C
<= 0.0100 torr
@Temperature 68.0 °F
AboCure
 <= 0.00133 bar
@Temperature 100 °C
<= 1.00 torr
@Temperature 212 °F
AboCast
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 65.5 MPa9500 psi
Modulus of Elasticity 3.447 GPa500.0 ksi
Flexural Yield Strength 96.53 MPa14000 psi
Compressive Yield Strength 103.4 MPa15000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.50e+16 ohm-cm>= 1.50e+16 ohm-cm
Dielectric Constant  3.6 - 3.8
@Frequency 1e+6 Hz
3.6 - 3.8
@Frequency 1e+6 Hz
 3.8 - 4.0
@Frequency 1000 Hz
3.8 - 4.0
@Frequency 1000 Hz
 3.9 - 4.1
@Frequency 50 Hz
3.9 - 4.1
@Frequency 50 Hz
Dielectric Strength 15.7 - 19.7 kV/mm
@Thickness 3.17 mm
400 - 500 kV/in
@Thickness 0.125 in
Short time value
Dissipation Factor  0.010 - 0.020
@Frequency 50 Hz
0.010 - 0.020
@Frequency 50 Hz
 0.010 - 0.020
@Frequency 1000 Hz
0.010 - 0.020
@Frequency 1000 Hz
 0.020 - 0.030
@Frequency 1e+6 Hz
0.020 - 0.030
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 - 95.0 µm/m-°C
@Temperature 20.0 °C
50.0 - 52.8 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.150 - 0.170 W/m-K1.04 - 1.18 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 55.0 °C131 °FDeflection temperature; load unknown.
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 °C77.0 °F
Pot Life  15.0 min
@Temperature 60.0 °C
15.0 min
@Temperature 140 °F
 30.0 min
@Temperature 40.0 °C
30.0 min
@Temperature 104 °F
 150 min
@Temperature 20.0 °C
150 min
@Temperature 68.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Electrically Conductive
Master Bond Supreme 10AOHT-LO High Shear and Peel Strength Epoxy
Master Bond EP42HT-2FG Two Component Epoxy Adhesive for Food Applications
Hybrid Plastics POSS® EP 1000 Epoxy Adhesive
Huntsman HY 3100 Aromatic Amine

PABER1 / 22017

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.