MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) Mackam® OCT-LS Surfactant  (discontinued **)
Categories: Fluid

Material Notes: Standard Applications: Mackam OCT-LS is a 50% active aqueous low-salt solution of octyl betaine. It acts as an effective hydrotrope to couple nonionic surfactant into high electrolyte systems. It can tolerate up to 25% sodium hydroxide and is a modest foamer. Mackam OCT-LS will not hydrolyze, even in strong mineral acids. It is useful for producing highly built cleaners with good detergency and high cloud points.

Chemical Name: Octyl Betaine

CAS No.: 27593-14-2

EINECS: 248-551-8

Information provided by Solvay. The Mackam® brand has been sold to Verdant Specialty Solutions, although this specific grade has been discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Solids Content 48 - 52 %48 - 52 %moisture balance; 150A
pH 5.0 - 7.05.0 - 7.0146A
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 3.0<= 3.0104A
 
Processing PropertiesMetricEnglishComments
Shelf Life 48.6 Month48.6 Month
 
Descriptive Properties
AppearanceClear liquid100C
Content<1%Free Amine, 236A
 <1%Ethanol, 510B
 <2%Sodium Chloride, 230B

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOLVAY735 / 218463

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.