MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Overview of materials for Polypropylene with 10% Glass Fiber Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Glass Fiber Filler

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.930 - 1.47 g/ccAverage value: 1.02 g/cc Grade Count:172
Filler Content 5.00 - 13.0 %Average value: 10.2 % Grade Count:58
Water Absorption 0.000 - 2.00 %Average value: 0.0864 % Grade Count:25
Additive Loading 5.00 - 10.0 %Average value: 9.29 % Grade Count:7
Linear Mold Shrinkage 0.00100 - 0.0390 cm/cmAverage value: 0.00734 cm/cm Grade Count:112
 0.00800 - 0.00800 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00800 cm/cm Grade Count:1
Linear Mold Shrinkage, Transverse 0.00620 - 0.0210 cm/cmAverage value: 0.0132 cm/cm Grade Count:13
 0.0120 - 0.0120 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.0120 cm/cm Grade Count:1
Melt Flow 1.00 - 31.0 g/10 minAverage value: 9.08 g/10 min Grade Count:125
Ash 10.0 - 32.0 %Average value: 14.3 % Grade Count:10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 76.0 - 110Average value: 89.5 Grade Count:33
Hardness, Shore D 32.0 - 73.0Average value: 68.6 Grade Count:28
Tensile Strength, Ultimate 20.0 - 170 MPaAverage value: 47.0 MPa Grade Count:107
Tensile Strength, Yield 21.0 - 114 MPaAverage value: 48.9 MPa Grade Count:60
Elongation at Break 2.00 - 100 %Average value: 7.60 % Grade Count:107
Elongation at Yield 2.00 - 10.0 %Average value: 4.41 % Grade Count:32
Modulus of Elasticity 1.70 - 9.40 GPaAverage value: 3.35 GPa Grade Count:72
Flexural Yield Strength 29.0 - 157 MPaAverage value: 61.5 MPa Grade Count:95
Flexural Modulus 0.900 - 15.0 GPaAverage value: 2.78 GPa Grade Count:157
Compressive Yield Strength 47.6 - 52.4 MPaAverage value: 49.1 MPa Grade Count:4
Izod Impact, Notched 0.267 - 3.74 J/cmAverage value: 0.762 J/cm Grade Count:119
Izod Impact, Unnotched 1.33 - 5340 J/cmAverage value: 4.47 J/cm Grade Count:41
Izod Impact, Notched (ISO) 4.50 - 24.0 kJ/m²Average value: 13.3 kJ/m² Grade Count:6
 10.0 - 10.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 10.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.00 - 7.70 J/cm²Average value: 4.27 J/cm² Grade Count:31
 1.90 - 5.50 J/cm²
@Temperature -50.0 - 0.000 °C
Average value: 3.05 J/cm² Grade Count:17
Charpy Impact, Notched 0.250 - 2.50 J/cm²Average value: 1.02 J/cm² Grade Count:44
 0.100 - 2.50 J/cm²
@Temperature -40.0 - 0.000 °C
Average value: 0.553 J/cm² Grade Count:27
Gardner Impact 0.339 - 9.94 JAverage value: 1.52 J Grade Count:31
 1.90 - 1.90 J
@Temperature -20.0 - -20.0 °C
Average value: 1.90 J Grade Count:1
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1000 - 1.00e+17 ohm-cmAverage value: 7.74e+15 ohm-cm Grade Count:29
Surface Resistance 10000 - 3.80e+15 ohmAverage value: 6.00e+14 ohm Grade Count:13
Static Decay 1.00 - 2.00 secAverage value: 1.83 sec Grade Count:6
Dielectric Constant 2.50 - 2.90Average value: 2.67 Grade Count:6
Dielectric Strength 19.3 - 40.1 kV/mmAverage value: 24.2 kV/mm Grade Count:12
Dissipation Factor 0.00100 - 0.00200Average value: 0.00114 Grade Count:7
Arc Resistance 80.0 - 132 secAverage value: 118 sec Grade Count:5
 
Thermal PropertiesOriginal ValueComments
CTE, linear 37.8 - 68.4 µm/m-°CAverage value: 55.0 µm/m-°C Grade Count:13
Thermal Conductivity 0.159 - 0.187 W/m-KAverage value: 0.180 W/m-K Grade Count:4
Melting Point 136 - 170 °CAverage value: 161 °C Grade Count:18
Deflection Temperature at 0.46 MPa (66 psi) 65.0 - 202 °CAverage value: 142 °C Grade Count:110
Deflection Temperature at 1.8 MPa (264 psi) 46.0 - 155 °CAverage value: 116 °C Grade Count:129
Vicat Softening Point 100 - 160 °CAverage value: 129 °C Grade Count:33
UL RTI, Electrical 65.0 °CAverage value: 65.0 °C Grade Count:5
UL RTI, Mechanical with Impact 65.0 °CAverage value: 65.0 °C Grade Count:5
UL RTI, Mechanical without Impact 65.0 °CAverage value: 65.0 °C Grade Count:5
Flammability, UL94 HB - V-0Grade Count:63
Glow Wire Test 550 - 960 °CAverage value: 753 °C Grade Count:7
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 260 °CAverage value: 214 °C Grade Count:18
Nozzle Temperature 191 - 260 °CAverage value: 222 °C Grade Count:37
Melt Temperature 60.0 - 270 °CAverage value: 217 °C Grade Count:78
Mold Temperature 20.0 - 90.0 °CAverage value: 47.3 °C Grade Count:99
Drying Temperature 60.0 - 220 °CAverage value: 85.7 °C Grade Count:69
Moisture Content 0.0500 - 0.200 %Average value: 0.0552 % Grade Count:29
Injection Pressure 2.76 - 130 MPaAverage value: 58.7 MPa Grade Count:60

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with 20% Glass Fiber Filler
Overview of materials for Polypropylene, Molded
Overview of materials for Polypropylene with 30% Glass Fiber Filler
Overview of materials for Polypropylene with 40% Glass Fiber Filler
Overview of materials for Polypropylene, Extrusion Grade

O4711 / 78376

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.