MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Aperam CuNi 2 Resistant Alloys Copper-Nickel Alloys
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: This alloy presents the particularity to be very malleable, to have a good resistance to corrosion until temperatures of 300°C and a good solderability. Ideal applications areas are all types of resistances used at low temperature.

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.90 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 300 MPa43500 psi
Tensile Strength, Yield 150 MPa21800 psi
Elongation at Break >= 25 %>= 25 %on 100 mm
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0000050 ohm-cm0.0000050 ohm-cmTemperature coefficient = 0.0013/°C from 20 - 100°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.4 µm/m-°C
@Temperature 20.0 - 1000 °C
8.00 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity 160 W/m-K
@Temperature 120 °C
1110 BTU-in/hr-ft²-°F
@Temperature 248 °F
Melting Point 1080 °C1980 °F
Maximum Service Temperature, Air 300 °C572 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 98 %98 %
Nickel, Ni 2.0 %2.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aperam CuNi 6 Resistant Alloys Copper-Nickel Alloys
Copper nickel 10%, UNS C70600
California Fine Wire Nico Copper Nickel Resistance Wire
Zirconium Copper (Amzirc Brand Copper), UNS C15000, 6 mm rod
Zirconium Copper (Amzirc Brand Copper), UNS C15000, 9.5 mm rod

NPERA097 / 194886

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.