MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zirconium Copper (Amzirc Brand Copper), UNS C15000, 9.5 mm rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent hot and cold workability. Fabricated by swaging, bending, heading, or forging.

Applications: Stud bases for power transmitters and rectifiers, switches and circuit breakers for high-temperature service, commutators, resistance welding tips and wheels, solderless wrapped connectors.

Test specimen: rod - 9.5mm diameter; cold worked 80% after solution treating (at 900-925°C), 44% after aging (1 hour or more at 400-425°C).

Key Words: ISO CuZr, CEN CW120C, N-4 Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7272TB04 or TH04 temper
Tensile Strength, Ultimate 470 MPa68200 psi
Tensile Strength, Yield 440 MPa63800 psi
Elongation at Break 11 %11 %in 50 mm
Modulus of Elasticity 129 GPa18700 ksi
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000186 ohm-cm
@Temperature 20.0 °C
0.00000186 ohm-cm
@Temperature 68.0 °F
solution treated, cold worked 84%, and aged material
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.9 µm/m-°C
@Temperature 20.0 - 100 °C
9.39 µin/in-°F
@Temperature 68.0 - 212 °F
 17.6 µm/m-°C
@Temperature 20.0 - 200 °C
9.78 µin/in-°F
@Temperature 68.0 - 392 °F
 20.2 µm/m-°C
@Temperature 20.0 - 300 °C
11.2 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Thermal Conductivity 367 W/m-K2550 BTU-in/hr-ft²-°FSolution treated, cold worked 84%, and aged material
Melting Point 980 - 1080 °C1800 - 1980 °F
Solidus 980 °C1800 °F
Liquidus 1080 °C1980 °F
Annealing Point 899 - 949 °C1650 - 1740 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 600 - 700 °C1110 - 1290 °F
Hot-Working Temperature 900 - 950 °C1650 - 1740 °F
Precipitation Temperature >= 499 °C
@Time 7200 sec
>= 930 °F
@Time 2.00 hour
Water
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 99.9 %99.9 %As Balance
Zirconium, Zr 0.050 - 0.15 %0.050 - 0.15 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zirconium Copper (Amzirc Brand Copper), UNS C15000, 6 mm rod
Zirconium Copper (Amzirc Brand Copper), UNS C15000, 13 mm rod
Zirconium Copper (Amzirc Brand Copper), UNS C15000, 2.3 mm wire, aged
Zirconium Copper (Amzirc Brand Copper), UNS C15000, 25 mm rod
Zirconium Copper (Amzirc Brand Copper), UNS C15000, 5 mm rod

MC15000b3 / 10634

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.