MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman DuraStar MN610 Polymer, Natural
Categories: Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Glycol-Modified PCT (PCTG) Copolyester

Material Notes: DuraStar™ Polymer MN610 Natural polymer has excellent appearance and is nearly water-clear. Benefits include toughness, chemical resistance, and excellent processing characteristics. MN610 has very good toughness as shown by Izod impact resistance. Easy to process, it flows readily and fills intricate molds. This product does not contain a mold release.

Applications/Uses

  • Blood Contact
  • Drug Delivery
  • IV Components
  • Medical
  • Surgical Instruments

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
@Thickness 3.20 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 103ASTM D785
Tensile Strength at Break 46.0 MPaISO 527
 51.0 MPaASTM D638
Tensile Strength, Yield 47.0 MPaASTM D638
 47.0 MPaISO 527
Elongation at Break 200 %ISO 527
 300 %ASTM D638
Elongation at Yield 4.0 %ISO 527
 5.0 %ASTM D638
Tensile Modulus 1.80 GPaISO 527
Flexural Strength 65.0 MPaISO 178
Flexural Yield Strength 69.0 MPaASTM D790
Flexural Modulus 1.85 GPaISO 178
 2.00 GPaASTM D790
Izod Impact, Notched 0.400 J/cm
@Temperature -40.0 °C
ASTM D256
 80.0 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched NBASTM D4812
 NB
@Temperature -40.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 4.80 kJ/m²
@Temperature -40.0 °C
ISO 180
 7.80 kJ/m²
@Temperature 23.0 °C
ISO 180
Puncture Energy 42.0 JPuncture Resistance @Max Load, 23°C; ASTM D3763
 48.0 J
@Temperature -40.0 °C
Puncture Resistance at Max Load; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 0.30 %ASTM D1003
Transmission, Visible 89 %Regular Transmittance; ASTM D1003
 91 %Total Transmittance; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 280 °C
Mold Temperature 15.0 - 30.0 °C
Drying Temperature 70.0 °C
Dry Time 3 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Eastar DN004 PCTG Copolyester
Eastman DuraStar DS1000 Polymer, Natural
A. Schulman ComAlloy Comtuf® 420 Polyester - PBT, High Impact Modified
Eastman DuraStar DS2000 Polymer, Natural
Eastman DuraStar DS1910HF Polymer, Natural

PE9012 / 35068

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.