Product Description: A super white opaque, cavitated BOPP film for Pressure Sensitive (PSA) labeling applications where superior optics are desired. 50LH247 also shows excellent performances on reel-fed wrap-around labeling machines, where its high stiffness is particularly appreciated. Availability: Africa & Middle East, Asia Pacific and Europe Key Features: - Outstanding white opaque background and superb white gloss finish
- Good printability on outside treated side
- Compatibility with most adhesive formulations
- Excellent stiffness and flex resistance
- Very good moisture resistance
- Good overall converting, diecutting and dispensing properties
Applications: - Dairy Products
- Industrial
Uses: - Pressure Sensitive Labels
- Reel-Fed Labels
Processing Method: Inner Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported, UV Flexographic Printing, UV Letterpress Printing, UV Offset Lithography Printing and Water-based Flexographic PrintingInformation provided by ExxonMobil |