MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Label-Lyte™ 50LH247 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A super white opaque, cavitated BOPP film for Pressure Sensitive (PSA) labeling applications where superior optics are desired. 50LH247 also shows excellent performances on reel-fed wrap-around labeling machines, where its high stiffness is particularly appreciated.

Availability: Africa & Middle East, Asia Pacific and Europe

Key Features:

  • Outstanding white opaque background and superb white gloss finish
  • Good printability on outside treated side
  • Compatibility with most adhesive formulations
  • Excellent stiffness and flex resistance
  • Very good moisture resistance
  • Good overall converting, diecutting and dispensing properties
Applications:
  • Dairy Products
  • Industrial
Uses:
  • Pressure Sensitive Labels
  • Reel-Fed Labels
Processing Method: Inner Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported, UV Flexographic Printing, UV Letterpress Printing, UV Offset Lithography Printing and Water-based Flexographic Printing

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milExxonMobil Method
Coating Weight 35.7 g/m²22.3 lb/reamExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 170 %170 %7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 55 %55 %7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Modulus of Elasticity 1.70 GPa247 ksiMD; ExxonMobil Method
 2.80 GPa406 ksiTD; ExxonMobil Method
Coefficient of Friction 0.600.60Untreated Surface; ExxonMobil Method
Film Tensile Strength at Break, MD 105 MPa15200 psi7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 185 MPa26800 psi7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 3.0 %
@Temperature 135 °C,
Time 432 sec
3.0 %
@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Shrinkage, TD 3.0 %
@Temperature 135 °C,
Time 432 sec
3.0 %
@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Gloss 70 %70 %45°; ExxonMobil Method
Transmission, Visible 22 %22 %ExxonMobil Method
 
Descriptive Properties
Yield19300 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kinlead PP11 Printing Grade BOPP Plain Film (thickness: 40 µm)

PEX99577 / 175813

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.