MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Evonik VESTAMID® LX9123 NC Nylon 12, 4% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 20% Glass Fiber Filled

Material Notes: VESTAMID® LX9123 NC is a high-viscosity, glass fiber-reinforced, heat and UV stabilized polyamide 12 compound with good process-ability for sport components such as shoe soles, which require very good fatigue performance. Parts made by the semi-crystalline polyamide VESTAMID® LX9123 NC are characterized by excellent dimensional stability, constantly high impact strength, low coefficient of friction, good chemical resistance at changing ambient humidity and excellent TPU bonding strength. The low melting point of VESTAMID® LX9123 NC enables especially the injection molding of parts with a wide processing window. It is suitable for applications with high ratio of flow length to wall thickness. Properties of compounds based on polyamide 12 vary little with changing humidity due to very low moisture absorption. VESTAMID® LX9123 NC is suitable for production of injection molded parts with efficient cycle times. VESTAMID® LX9123 NC is supplied as cylindrical granules ready for processing, in moisture-proof bags. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Dry properties listed below
Industrial Sector: Sustainable, Sports and Lifestyle
Sustainability: Sustainable electricity
Processing: Injection molding
Delivery form: Pellets, Granules
Optics: Translucent
Resistance to: Fatigue resistance
Electrical: Insulating
Additives: Glass fibers
Applications: General purpose
Special Characteristics: Semi-crystalline, Light-stabilized, U.V. stabilized
Features: Lightweight
Color: Natural color
Additives: Antioxidant agent, Light stabilizer
Delivery form: Cylindrical pellets

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.00800 cm/cm0.00800 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.00500 cm/cm0.00500 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75.075.0ISO 7619-1
Tensile Strength at Break 34.0 MPa4930 psiISO 527
Tensile Strength, Yield 52.0 MPa7540 psiISO 527
Elongation at Break >= 50.0 %>= 50.0 %Nominal; ISO 527
Elongation at Yield 4.80 %4.80 %ISO 527
Tensile Modulus 1.79 GPa260 ksiISO 527
Flexural Modulus 1.40 GPa203 ksiISO 178
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²Type of failure: C; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 °C352 °FISO 11357-1/-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 °C464 °F
Mold Temperature 60.0 °C140 °F
 
Descriptive Properties
Blue water consumption238.4 kgISO 14040, 14044
ColorNatural Color
Global Warming Potential1.9 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 6.1 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
 6.4 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)3.0 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7930 / 325062

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.