MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 85 P 4380 TPU-Polyether
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Introduction: IROGRAN A 85 P 4380 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of the product are excellent microbial resistance, high low-temperature flexibility, especially suitable for cable jackets.

Performance Features:

  • Excellent hydrolysis resistance
  • High microbial resistance
  • Low-adhesion surfaces
  • Flame retardant
  • Halogen-free
  • Good melt flow
  • UL 94 classification V2
Applications:
  • Cables
  • Hoses
  • Profiles
  • Cable Bushings

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccASTM D792
Linear Mold Shrinkage 0.0080 in/inASTM D995
Melt Flow 30 - 60 g/10 minMelt Volume Rate (cm³/10 min)
Melt Index of Compound 50 g/10 min
@Load 21.6 kg,
Temperature 190 °C
cm3/10 min
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 87ASTM D2240
Hardness, Shore D 36ASTM D2240
Tensile Strength at Break 35.0 MPaDIN 53504
Elongation at Break 610 %ASTM D412
100% Modulus 0.00650 GPa
@Strain 100 %
DIN 53504
300% Modulus 0.0100 GPa
@Strain 300 %
DIN 53504
Rebound 42 %Bayshore; ASTM D2632
Tear Strength 460 pliASTM D624
Abrasion 35[mm3]; ISO 4649
Compression Set 25 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM D395
 45 %
@Temperature 70.0 °C,
Time 86400 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Melting Point 159 - 180 °CHuntsman/TMA
Flammability, UL94 V-2Non-Halogen FR
 
Processing PropertiesOriginal ValueComments
Feed Temperature 25.0 - 40.0 °CExtrusion
Front Barrel Temperature 165 - 190 °CExtrusion
Nozzle Temperature 170 - 200 °CExtrusion
 180 - 200 °CInjection
Adapter Temperature 175 - 195 °CExtrusion
Die Temperature 175 - 200 °CExtrusion
Melt Temperature 170 - 195 °CInjection
Mold Temperature 20.0 - 70.0 °CInjection
 
Descriptive Properties
Heating Zone175-195°CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 65 P 4324 N TPU-Polyether
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether
Huntsman IROGRAN® A 75 P 4665N TPU-Polyether
Huntsman IROGRAN® A 78 P 4766 TPU-Polyether
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether

PHU9928 / 150388

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.