MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Astro Met AmZirOx 86 Zirconia - Zirconium Oxide
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: AmZirOx 86 zirconia (Astro Met Zirconium Oxide) is a yttria stabilized zirconia ceramic material which features high strength and toughness making it a candidate material for use in severe structural applications which exhibit wear, corrosion, abrasion and impact. This material is also commonly referred to as Y-TZP or Yttria Tetragonal Zirconia Polycrystal. AmZirOx 86 zirconia has been developed with a unique micro structure utilizing transformation toughening which allows AmZirOx 86 zirconia to absorb the energy of impacts that would cause most ceramics to fail.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.01 g/cc
Water Absorption 0.00 %
Particle Size 0.50 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 1290
Modulus of Elasticity 204 GPa
Flexural Strength 1000 MPa
Poissons Ratio 0.31
Fracture Toughness 7.00 MPa-m½
Shear Modulus 77.8 GPaCalculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.3 µm/m-°C
@Temperature 25.0 - 1000 °C
Specific Heat Capacity 0.320 BTU/lb-°F
Thermal Conductivity 15.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 2400 °Cno load
 
Component Elements PropertiesOriginal ValueComments
Y2O3 5.0 %
ZrO2 95 %
 
Descriptive Properties
ColorIvory
Gas Permeation, %0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for AISI 1000 Series Steel
Overview of materials for Nickel Alloy
Zirconium Oxide, Zirconia, ZrO2
Overview of materials for Beryllium Alloy
Overview of materials for Copper Alloy

CASTR02 / 630

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.