MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Overview of materials for Beryllium Alloy
Categories: Metal; Nonferrous Metal; Beryllium Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Beryllium Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.84 - 23.1 g/cc0.0665 - 0.836 lb/in³Average value: 7.84 g/cc Grade Count:405
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 190 - 380190 - 380Average value: 256 Grade Count:9
Hardness, Rockwell B 20.0 - 10620.0 - 106Average value: 81.2 Grade Count:169
Hardness, Rockwell C 20.0 - 10020.0 - 100Average value: 37.4 Grade Count:108
Hardness, Rockwell 30T 62.0 - 83.062.0 - 83.0Average value: 75.3 Grade Count:3
Hardness, Vickers 65.0 - 69565.0 - 695Average value: 272 Grade Count:107
Tensile Strength, Ultimate 175 - 2550 MPa25400 - 370000 psiAverage value: 828 MPa Grade Count:382
Tensile Strength, Yield 60.0 - 1690 MPa8700 - 245000 psiAverage value: 684 MPa Grade Count:380
Elongation at Break 0.600 - 75.0 %0.600 - 75.0 %Average value: 13.9 % Grade Count:378
Modulus of Elasticity 0.138 - 330 GPa20.0 - 47900 ksiAverage value: 149 GPa Grade Count:386
Compressive Yield Strength 147 - 1200 MPa21300 - 174000 psiAverage value: 731 MPa Grade Count:14
Poissons Ratio 0.0320 - 0.3300.0320 - 0.330Average value: 0.228 Grade Count:65
Fatigue Strength 0.276 - 552 MPa40.0 - 80100 psiAverage value: 268 MPa Grade Count:97
Fracture Toughness 7.30 - 23.9 MPa-m½6.64 - 21.8 ksi-in½Average value: 12.0 MPa-m½ Grade Count:9
Machinability 10.0 - 60.0 %10.0 - 60.0 %Average value: 31.5 % Grade Count:81
Shear Modulus 41.0 - 135 GPa5950 - 19600 ksiAverage value: 83.6 GPa Grade Count:65
Shear Strength 181 - 480 MPa26300 - 69600 psiAverage value: 298 MPa Grade Count:5
Charpy Impact 1.50 - 67.8 J1.11 - 50.0 ft-lbAverage value: 20.5 J Grade Count:6
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000250 - 0.0000907 ohm-cm0.00000250 - 0.0000907 ohm-cmAverage value: 0.0000109 ohm-cm Grade Count:377
Magnetic Permeability 1.00 - 1.001.00 - 1.00Average value: 1.00 Grade Count:5
Magnetic Susceptibility -1.00e-6-1.00e-6Average value: -1.00e-6 Grade Count:23
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.50 - 18.4 µm/m-°C3.61 - 10.2 µin/in-°FAverage value: 16.6 µm/m-°C Grade Count:373
Specific Heat Capacity 0.377 - 1.92 J/g-°C0.0900 - 0.460 BTU/lb-°FAverage value: 1.00 J/g-°C Grade Count:80
Thermal Conductivity 17.3 - 300 W/m-K120 - 2080 BTU-in/hr-ft²-°FAverage value: 146 W/m-K Grade Count:362
Melting Point 585 - 1330 °C1090 - 2430 °FAverage value: 995 °C Grade Count:323
Solidus 644 - 1200 °C1190 - 2200 °FAverage value: 951 °C Grade Count:247
Liquidus 585 - 1330 °C1090 - 2430 °FAverage value: 1040 °C Grade Count:249
Boiling Point 2470 °C4480 °FAverage value: 2470 °C Grade Count:23
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.6100.610Average value: 0.610 Grade Count:23
Reflection Coefficient, Visible (0-1) 0.5000.500Average value: 0.500 Grade Count:23
 
Processing PropertiesMetricEnglishComments
Processing Temperature 450 - 980 °C842 - 1800 °FAverage value: 845 °C Grade Count:14
Annealing Temperature 760 - 790 °C1400 - 1450 °FAverage value: 775 °C Grade Count:4
Solution Temperature 760 - 1090 °C1400 - 2000 °FAverage value: 871 °C Grade Count:36
Aging Temperature 260 - 510 °C500 - 950 °FAverage value: 415 °C Grade Count:36
Hot-Working Temperature 650 - 925 °C1200 - 1700 °FAverage value: 779 °C Grade Count:12
Precipitation Temperature 316 - 482 °C600 - 900 °FAverage value: 416 °C Grade Count:10
Casting Temperature 980 - 1480 °C1800 - 2700 °FAverage value: 1140 °C Grade Count:33
Recrystallization Temperature 730 °C1350 °FAverage value: 730 °C Grade Count:4
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.0100 - 97.8 %0.0100 - 97.8 %Average value: 12.6 % Grade Count:58
BeO 0.0300 - 73.2 %0.0300 - 73.2 %Average value: 7.70 % Grade Count:23
Beryllium, Be 0.150 - 100 %0.150 - 100 %Average value: 11.1 % Grade Count:380
Boron, B 0.000200 - 0.000300 %0.000200 - 0.000300 %Average value: 0.000260 % Grade Count:5
Cadmium, Cd 0.000200 %0.000200 %Average value: 0.000200 % Grade Count:5
Calcium, Ca 0.00500 - 0.0200 %0.00500 - 0.0200 %Average value: 0.0144 % Grade Count:8
Carbon, C 0.0300 - 2.00 %0.0300 - 2.00 %Average value: 0.193 % Grade Count:26
Chromium, Cr 0.00250 - 96.2 %0.00250 - 96.2 %Average value: 3.17 % Grade Count:41
Co + Ni 0.200 - 3.00 %0.200 - 3.00 %Average value: 0.269 % Grade Count:175
Co + Ni + Fe 0.600 %0.600 %Average value: 0.600 % Grade Count:155
Cobalt, Co 0.000500 - 2.70 %0.000500 - 2.70 %Average value: 1.62 % Grade Count:96
Copper, Cu 0.00500 - 99.5 %0.00500 - 99.5 %Average value: 90.3 % Grade Count:336
Germanium, Ge 0.200 - 0.950 %0.200 - 0.950 %Average value: 0.383 % Grade Count:3
Iron, Fe 0.0300 - 0.400 %0.0300 - 0.400 %Average value: 0.155 % Grade Count:59
Lead, Pb 0.000500 - 0.600 %0.000500 - 0.600 %Average value: 0.0927 % Grade Count:106
Lithium, Li 0.000300 %0.000300 %Average value: 0.000300 % Grade Count:4
Magnesium, Mg 0.00600 - 0.500 %0.00600 - 0.500 %Average value: 0.108 % Grade Count:22
Manganese, Mn 0.00300 - 0.0200 %0.00300 - 0.0200 %Average value: 0.0111 % Grade Count:9
Molybdenum, Mo 0.00100 - 0.00500 %0.00100 - 0.00500 %Average value: 0.00213 % Grade Count:8
Nickel, Ni 0.0200 - 97.7 %0.0200 - 97.7 %Average value: 23.1 % Grade Count:112
Nitrogen, N 0.0300 - 0.0400 %0.0300 - 0.0400 %Average value: 0.0325 % Grade Count:4
Oxygen, O 0.240 - 46.8 %0.240 - 46.8 %Average value: 14.4 % Grade Count:7
Silicon, Si 0.0100 - 2.50 %0.0100 - 2.50 %Average value: 0.206 % Grade Count:51
Silver, Ag 0.000500 - 3.35 %0.000500 - 3.35 %Average value: 0.494 % Grade Count:15
Tin, Sn 0.100 - 0.250 %0.100 - 0.250 %Average value: 0.121 % Grade Count:29
Titanium, Ti 0.00100 - 0.600 %0.00100 - 0.600 %Average value: 0.398 % Grade Count:23
Zinc, Zn 0.00500 - 0.100 %0.00500 - 0.100 %Average value: 0.0864 % Grade Count:32
Zirconium, Zr 0.0100 - 0.500 %0.0100 - 0.500 %Average value: 0.349 % Grade Count:8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nickel Alloy
Overview of materials for Stainless Steel
Overview of materials for Aluminum Alloy
Overview of materials for Copper Alloy
Overview of materials for T 300 Series Stainless Steel

M01048 / 81666

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.