MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Celanese Celanex® 2012 Polyester (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Flame Retardant

Material Notes: Flame retardant

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ASTM D792
Water Absorption 0.090 %0.090 %ASTM D570
Linear Mold Shrinkage, Flow 0.019 cm/cm0.019 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8080ISO 2039-2
Tensile Strength, Yield 60.0 MPa8700 psiISO 527
Elongation at Break 24 %24 %ASTM D638
Flexural Strength 95.0 MPa13800 psiISO 178
Flexural Modulus 2.70 GPa392 ksiISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.2
@Frequency 100 Hz
3.2
@Frequency 100 Hz
Dielectric Strength 18.0 kV/mm
@Thickness 3.17 mm
457 kV/in
@Thickness 0.125 in
50% RH; ASTM D149
Dissipation Factor 0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
Comparative Tracking Index 250 V250 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 152 °C306 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C135 °FISO 75
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
UL94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celanex® 4016 PBT, Unfilled
Celanese Celanex® 1300A Polyester (PBT)
Celanese Celanex® 2016 PBT, Unfilled
Celanese Celanex® XFR 4840 PBT, Unfilled
Celanese Celanex® 2014 Flame Retarded Unreinforced Polybutylene Terephthalate

PHCT11 / 45651

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.