MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celanex® 2014 Flame Retarded Unreinforced Polybutylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Flame Retardant

Material Notes: Description: Celanex 2014 is a non-exuding flame retarded (UL approved V-0 at 1/32 inch), unreinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is well suited for electrical connector applications.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³ISO 1183 & ASTM D792
Linear Mold Shrinkage 0.023 - 0.025 cm/cm0.023 - 0.025 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7979ISO 2039-2
Tensile Strength, Yield 64.0 MPa9280 psi50 mm/min; ISO 527-2/1A
Elongation at Break 12 %12 %50 mm/min; ISO 527-2/1A
Elongation at Yield 7.0 %7.0 %50 mm/min; ISO 527-2/1A
Tensile Modulus 3.00 GPa435 ksi1 mm/min; ISO 527-2/1A
Flexural Strength 90.0 MPa13100 psiISO 178
Flexural Modulus 3.00 GPa435 ksiISO 178
Izod Impact, Notched (ISO) 4.50 kJ/m²2.14 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmIEC 60093
Surface Resistance >= 1.00e+17 ohm>= 1.00e+17 ohmIEC 60093
Dielectric Constant  3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
IEC 60250
 3.6
@Frequency 100 Hz
3.6
@Frequency 100 Hz
IEC 60250
Dielectric Strength 37.0 kV/mm940 kV/inIEC 60243-1
Dissipation Factor  0.0047
@Frequency 100 Hz
0.0047
@Frequency 100 Hz
IEC 60250
 0.0185
@Frequency 1e+6 Hz
0.0185
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 325 V325 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 139 µm/m-°C
@Temperature 20.0 °C
77.2 µin/in-°F
@Temperature 68.0 °F
ISO 11359-2
Melting Point 225 °C437 °FISO 11357-1,2,3 & ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 134 °C273 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C151 °FISO 75-1, -2
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 240 °C446 - 464 °F
Middle Barrel Temperature 235 - 250 °C455 - 482 °F
Front Barrel Temperature 240 - 255 °C464 - 491 °F
Nozzle Temperature 250 - 255 °C482 - 491 °F
Melt Temperature 235 - 255 °C455 - 491 °F
Mold Temperature 65.0 - 93.0 °C149 - 199 °F
Drying Temperature 121 °C250 °F
Dry Time 4 hour4 hour
Back Pressure 0.000 - 0.345 MPa0.000 - 50.0 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celanex® 2300 GV1/30 PBT, 30% Glass Reinforced
Celanese Celanex® 3316CT PBT, 50% Glass Reinforced
Celanese Celanex® XFR 6842 GF20 PBT, 30% Glass Reinforced
Celanese Celanex® XFR 4840 PBT, Unfilled
Celanese Celanex® 4016 PBT, Unfilled

PHCV70 / 45911

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.