Applications- Launder linings
- Lining of distribution launders for DC casting table
- Industrial furnace linings
- Back up material behind hot face lining
Advantages - Low density with high insulating properties
- Non-wetting to molten aluminum
- Easy to handle
- Saves drying time
- Immediate heating for drying is possible just after molding
Information provided by Pyrotek. |