MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek Pyromoldable JDR1150A Moldable Paste Type Low Density Refractory
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Applications
  • Launder linings
  • Lining of distribution launders for DC casting table
  • Industrial furnace linings
  • Back up material behind hot face lining

Advantages

  • Low density with high insulating properties
  • Non-wetting to molten aluminum
  • Easy to handle
  • Saves drying time
  • Immediate heating for drying is possible just after molding

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 1.96 - 2.94 MPa284 - 426 psiTransverse
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.116 W/m-K
@Temperature 500 °C
0.805 BTU-in/hr-ft²-°F
@Temperature 932 °F
Maximum Service Temperature, Air 1300 °C2370 °F
Shrinkage 0.60 - 0.80 %
@Temperature 800 °C,
Time 3600 sec
0.60 - 0.80 %
@Temperature 1470 °F,
Time 1.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Pyrocast SC-2600 Castable Refractory
Pyrotek Pyrocast XL Small Component Refractory
Pyrotek S-679 Dense Graphite Material Treated for Oxidation Resistance
Pyrotek Pyrocast ZE Refractory Shapes
Pyrotek Pyrocast ZC Refractory Shapes

CPYRO205 / 1922

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.