Product description: TEGOMER® V-Si 4042 is a solvent free, reactive polysiloxane to be used as additive for thermo-plastic compounds as well as for EPDM compounds with peroxide curing. Application: TEGOMER® V-Si 4042 serves as process aid for highly loaded compounds containing carbon black or mineral fillers, like aluminum or magnesium hydroxide. TEGOMER® V-Si 4042 enhances the flame retardant properties of the compound. TEGOMER® V-Si 4042 can be used to produce halogen free flame retardant polyolefin and elastomeric compounds for cable application. By thermally initiated crosslinking reactions TEGOMER® V-Si 4042 can be introduced permanently into polymeric resins and is therefore even suitable for x-PE application. TEGOMER® V-Si 4042 is a process aid which improves the extrusion of EPM/EPDM compounds without changes in physical properties of the rubber article. Benefits: TEGOMER® V-Si 4042 provides several benefits to the HFFR polymer formulation such as: - improved polymer processing and lubrication of polymer resin
- excellent compatibilizing of (high addition levels of) inorganic fillers in the polymeric resin
- improved melt flow rates during processing
- excellent surface characteristics of cables
- no build-up of process aid on metal surfaces and no die drol appears
- excellent char formation
- low smoking cable formulation can be achieved
- low heat and smoke release
- significant improved Lower Oxygen Index (LOI)
TEGOMER® V-Si 4042 provides several benefits to EPM/EPDM peroxide cured compounds:- reduces the compound viscosity at higher shear forces for increased capacity or for reduced energy cost
- does not change mechanical properties as other process aids usually do
- reduces failures on the extruded surface
Information provided by Evonik |