MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik TEGOMER® V-Si 4042 Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product description: TEGOMER® V-Si 4042 is a solvent free, reactive polysiloxane to be used as additive for thermo-plastic compounds as well as for EPDM compounds with peroxide curing.

Application: TEGOMER® V-Si 4042 serves as process aid for highly loaded compounds containing carbon black or mineral fillers, like aluminum or magnesium hydroxide. TEGOMER® V-Si 4042 enhances the flame retardant properties of the compound. TEGOMER® V-Si 4042 can be used to produce halogen free flame retardant polyolefin and elastomeric compounds for cable application. By thermally initiated crosslinking reactions TEGOMER® V-Si 4042 can be introduced permanently into polymeric resins and is therefore even suitable for x-PE application. TEGOMER® V-Si 4042 is a process aid which improves the extrusion of EPM/EPDM compounds without changes in physical properties of the rubber article.

Benefits: TEGOMER® V-Si 4042 provides several benefits to the HFFR polymer formulation such as:

  • improved polymer processing and lubrication of polymer resin
  • excellent compatibilizing of (high addition levels of) inorganic fillers in the polymeric resin
  • improved melt flow rates during processing
  • excellent surface characteristics of cables
  • no build-up of process aid on metal surfaces and no die drol appears
  • excellent char formation
  • low smoking cable formulation can be achieved
  • low heat and smoke release
  • significant improved Lower Oxygen Index (LOI)
TEGOMER® V-Si 4042 provides several benefits to EPM/EPDM peroxide cured compounds:
  • reduces the compound viscosity at higher shear forces for increased capacity or for reduced energy cost
  • does not change mechanical properties as other process aids usually do
  • reduces failures on the extruded surface

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
Viscosity 1500 cP1500 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 300 °C>= 572 °F
 
Descriptive Properties
Appearancecolorless, clear
Content100%Active matter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
5250 Aluminum Composition Spec

PEVONIL593 / 196797

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.