MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik VESTAMID® L2124 BK 9.7507 Nylon 12, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® L2124 BK 9.7507 is a plasticized, heat- and light- stabilized polyamide 12 compound for the extrusion of flexible tubing and hoses especially for oil and petrochemical applications. Tubing according to DIN 73 378, Type: PA 12-PHL. Properties of compounds based on PA 12 vary little with changing humidity due to low moisture absorption. Parts made of this semi-crystalline material are characterized by exceptional impact strength, low coefficient of friction and good chemical resistance. VESTAMID® L2124 BK 9.7507 is characterized by a high melt viscosity and good dimensional control during pipe extrusion. VESTAMID® L2124 BK 9.7507 is supplied as cylindrical granules, ready for processing, in moisture-proof bags. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Industrial Sector: Automotive and Mobility, Sustainable, Industry and Engineering
Sustainability: Sustainable electricity
Processing: Injection molding, Extrusion
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels
Electrical: Insulating
Conformity: Automotive
Additives: Lubricant, Unfilled
Processing: Profile extrusion, Pipe/Tube extrusion
Special Characteristics: Semi-crystalline, Light-stabilized, U.V. stabilized, High heat resistant
Features: Low coefficient of friction
Color: Black
Additives: Plasticizer, Light stabilizer, Heat stabilizer, Processing aids
Chemical Resistance: Oil resistance, General chemical resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ISO 1183
Water Absorption 1.30 %1.30 %Sim to ISO 62
Moisture Absorption 0.500 %0.500 %Sim to ISO 62
Linear Mold Shrinkage, Flow 0.00700 cm/cm0.00700 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0130 cm/cm0.0130 in/inISO 294-4, 2577
Melt Flow 9.00 g/10 min
@Load 5.00 kg,
Temperature 230 °C
9.00 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 42.0 MPa6090 psiISO 527
Tensile Strength 28.0 MPa4060 psiISO 527
Tensile Stress 28.0 MPa
@Strain 50.0 %
4060 psi
@Strain 50.0 %
ISO 527
 9.00 MPa
@Strain 10.0 %,
Temperature 120 °C
1310 psi
@Strain 10.0 %,
Temperature 248 °F
 10.0 MPa
@Strain 10.0 %,
Temperature 100 °C
1450 psi
@Strain 10.0 %,
Temperature 212 °F
 10.0 MPa
@Strain 50.0 %,
Temperature 120 °C
1450 psi
@Strain 50.0 %,
Temperature 248 °F
 13.0 MPa
@Strain 10.0 %,
Temperature 80.0 °C
1890 psi
@Strain 10.0 %,
Temperature 176 °F
 15.0 MPa
@Strain 10.0 %,
Temperature 60.0 °C
2180 psi
@Strain 10.0 %,
Temperature 140 °F
 15.0 MPa
@Strain 50.0 %,
Temperature 100 °C
2180 psi
@Strain 50.0 %,
Temperature 212 °F
 17.0 MPa
@Strain 50.0 %,
Temperature 80.0 °C
2470 psi
@Strain 50.0 %,
Temperature 176 °F
 20.0 MPa
@Strain 9.00 %,
Temperature 23.0 °C
2900 psi
@Strain 9.00 %,
Temperature 73.4 °F
 20.0 MPa
@Strain 15.0 %,
Temperature 40.0 °C
2900 psi
@Strain 15.0 %,
Temperature 104 °F
 20.0 MPa
@Strain 50.0 %,
Temperature 60.0 °C
2900 psi
@Strain 50.0 %,
Temperature 140 °F
 20.0 MPa
@Strain 1.00 %,
Temperature -40.0 °C
2900 psi
@Strain 1.00 %,
Temperature -40.0 °F
Yield
 20.0 MPa
@Strain 2.00 %,
Temperature -20.0 °C
2900 psi
@Strain 2.00 %,
Temperature -4.00 °F
Yield
 20.0 MPa
@Strain 4.00 %,
Temperature 0.000 °C
2900 psi
@Strain 4.00 %,
Temperature 32.0 °F
Yield
 23.0 MPa
@Strain 50.0 %,
Temperature 40.0 °C
3340 psi
@Strain 50.0 %,
Temperature 104 °F
 25.0 MPa
@Strain 50.0 %,
Temperature 23.0 °C
3630 psi
@Strain 50.0 %,
Temperature 73.4 °F
 35.0 MPa
@Strain 25.0 %,
Temperature 0.000 °C
5080 psi
@Strain 25.0 %,
Temperature 32.0 °F
Yield
 50.0 MPa
@Strain 20.0 %,
Temperature -20.0 °C
7250 psi
@Strain 20.0 %,
Temperature -4.00 °F
Yield
 65.0 MPa
@Strain 10.0 %,
Temperature -40.0 °C
9430 psi
@Strain 10.0 %,
Temperature -40.0 °F
Yield
Tensile Strength, Yield 28.0 MPa4060 psiISO 527
Elongation at Break 210 %210 %Nominal; ISO 527
Elongation at Yield 33.0 %33.0 %ISO 527
Tensile Modulus 0.400 GPa58.0 ksiISO 527
Flexural Modulus 0.400 GPa58.0 ksiISO 178
Secant Modulus  0.0400 GPa
@Strain 50.0 %,
Temperature 120 °C
5.80 ksi
@Strain 50.0 %,
Temperature 248 °F
 0.0500 GPa
@Strain 50.0 %,
Temperature 100 °C
7.25 ksi
@Strain 50.0 %,
Temperature 212 °F
 0.0600 GPa
@Strain 50.0 %,
Temperature 80.0 °C
8.70 ksi
@Strain 50.0 %,
Temperature 176 °F
 0.0700 GPa
@Strain 50.0 %,
Temperature 60.0 °C
10.2 ksi
@Strain 50.0 %,
Temperature 140 °F
 0.0800 GPa
@Strain 50.0 %,
Temperature 40.0 °C
11.6 ksi
@Strain 50.0 %,
Temperature 104 °F
 0.0900 GPa
@Strain 50.0 %,
Temperature 23.0 °C
13.1 ksi
@Strain 50.0 %,
Temperature 73.4 °F
 0.100 GPa
@Strain 2.00 %,
Temperature 120 °C
14.5 ksi
@Strain 2.00 %,
Temperature 248 °F
 0.150 GPa
@Strain 2.00 %,
Temperature 100 °C
21.8 ksi
@Strain 2.00 %,
Temperature 212 °F
 0.200 GPa
@Strain 2.00 %,
Temperature 80.0 °C
29.0 ksi
@Strain 2.00 %,
Temperature 176 °F
 0.200 GPa
@Strain 25.0 %,
Temperature 0.000 °C
29.0 ksi
@Strain 25.0 %,
Temperature 32.0 °F
Yield
 0.250 GPa
@Strain 2.00 %,
Temperature 60.0 °C
36.3 ksi
@Strain 2.00 %,
Temperature 140 °F
 0.300 GPa
@Strain 2.00 %,
Temperature 40.0 °C
43.5 ksi
@Strain 2.00 %,
Temperature 104 °F
 0.300 GPa
@Strain 20.0 %,
Temperature -20.0 °C
43.5 ksi
@Strain 20.0 %,
Temperature -4.00 °F
Yield
 0.350 GPa
@Strain 2.00 %,
Temperature 23.0 °C
50.8 ksi
@Strain 2.00 %,
Temperature 73.4 °F
 0.750 GPa
@Strain 10.0 %,
Temperature -40.0 °C
109 ksi
@Strain 10.0 %,
Temperature -40.0 °F
Yield
 0.750 GPa
@Strain 1.00 %,
Temperature 0.000 °C
109 ksi
@Strain 1.00 %,
Temperature 32.0 °F
Yield
 1.25 GPa
@Strain 1.00 %,
Temperature -20.0 °C
181 ksi
@Strain 1.00 %,
Temperature -4.00 °F
Yield
 2.40 GPa
@Strain 0.000 %,
Temperature -40.0 °C
348 ksi
@Strain 0.000 %,
Temperature -40.0 °F
Yield
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 15.0 J/cm²
@Temperature 23.0 °C
71.4 ft-lb/in²
@Temperature 73.4 °F
Type of failure: P; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 62631-3-1
Dielectric Constant  3.80
@Frequency 1.00e+6 Hz
3.80
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 12.0
@Frequency 100 Hz
12.0
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 32.0 kV/mm813 kV/inAC, S20/P50; Sim. To IEC 60243-1
 37.0 kV/mm940 kV/inAC, S20/S20, t.; IEC 60243-1
Dissipation Factor  0.150
@Frequency 1.00e+6 Hz
0.150
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 0.160
@Frequency 100 Hz
0.160
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 600 V600 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 170 µm/m-°C
@Temperature 25.0 - 55.0 °C
94.4 µin/in-°F
@Temperature 77.0 - 131 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 160 µm/m-°C
@Temperature 25.0 - 55.0 °C
88.9 µin/in-°F
@Temperature 77.0 - 131 °F
ISO 11359-1/-2
Melting Point 171 °C340 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C208 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FISO 75-1/-2
Vicat Softening Point  125 °C
@Load 5.10 kg
257 °F
@Load 11.2 lb
50 K/h; ISO 306
 165 °C
@Load 1.02 kg
329 °F
@Load 2.25 lb
50 K/h; ISO 306
Flammability, UL94  HB
@Thickness 1.30 mm
HB
@Thickness 0.0512 in
IEC 60695-11-10
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 °C428 °FInjection Molding; ISO 294
 220 °C428 °F
Mold Temperature 60.0 °C140 °F
 60.0 °C140 °FInjection Molding; ISO 294
Injection Velocity 200 mm/sec7.87 in/secInjection Molding; ISO 294
Injection Pressure 70.0 MPa10200 psiInjection Molding; ISO 294
 
Descriptive Properties
Blue water consumption25.9 kgISO 14040, 14044
ColorBlack
Global Warming Potential2.6 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 5.7 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
 5.8kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.3 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7906 / 325038

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.